Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 106 MPa | 15400 psi | ISO 527-2 |
PolyOne Edgetek® NJ-30GF/000 natural Polyamide 12 (Nylon 12) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Strength, Yield | 106 MPa | 15400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DFL146 PC (Europe-Africa-Middle East) LNP* Lubricomp* DFL146 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Flame Retardant. |
|||
Tensile Strength, Yield | 106 MPa | 15400 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP COLORCOMP EX10304C PEI (Asia Pacific) LNP* Colorcomp* EX10304C is an unfilled polyetherimide clean compound with extremely high level of cleanliness for the most demanding application. This compound is manufactured using LNP CCS Technol.. |
|||
Tensile Strength, Yield | 106 MPa | 15400 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP EX03599H PEI LNP* LUBRICOMP* EX03599H is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Healthcare, Wear Resistant. |
|||
Tensile Strength, Yield | 106 MPa | 15400 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT LNP* Lubricomp* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Ret.. |
|||
Tensile Strength, Yield | 106 MPa | 15400 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT (Asia Pacific) LNP* Lubricomp* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Ret.. |
|||
Tensile Strength, Yield | 106 MPa | 15400 psi | ASTM D638 |
Techmer ES HiFill® PA4/6 0206 Availability: North AmericaForms: PelletsFeatures: High Specific Gravity and Thermally ConductiveInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 106 MPa | 15400 psi | SABIC - Japan Method |
SABIC Innovative Plastics Valox® VIC4350 PBT (Asia Pacific) |
|||
Tensile Strength, Yield | 106 MPa | 15400 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON Noryl_NC2525 PPE+HIPS (Europe-Africa-Middle East) LNP* Stat-kon* Noryl_NC2525 compound is a 25% CFR PPE+PS. Highly conductive. High heat. May be added to similar material/regrind to add some conductivity to the blend. |
|||
Tensile Strength, Yield | 106 MPa | 15400 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON Noryl_NC2525 PPE+PS LNP* Stat-kon* Noryl_NC2525 compound is a 25% CFR PPE+PS. Highly conductive. High heat. May be added to similar material/regrind to add some conductivity to the blend. |
|||
Tensile Strength, Yield | 106 MPa | 15400 psi | ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP EX06430H PEI LNP* THERMOCOMP* EX06430H is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added feature of this grade is: Healthcare. |
|||
Tensile Strength, Yield | 106 MPa | 15400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PCN2910 PPE+PS LNP* Thermodcomp* Noryl_PCN2910 compound is a 35% Glass/Mica filled. High modulus and tight tolerance molding for the chassis market. |
|||
Tensile Strength, Yield | 106 MPa | 15400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PCN2910 PPE+PS (Asia Pacific) 35% Glass/Mica filled. High modulus and tight tolerance molding for the chassis market. |
|||
Tensile Strength, Yield | 106 MPa | 15400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PCN2910 PPE+PS (Asia Pacific) 35% Glass/Mica filled. High modulus and tight tolerance molding for the chassis market. |
|||
Tensile Strength, Yield | 106 MPa @Temperature 149 °C |
15400 psi @Temperature 300 °F |
ASTM D638 |
Mitsui AURUM® JGN3030 Polyimide, Glass Fiber Filled