Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1034 - 1207 MPa | 150000 - 175100 psi | |
Materion Beryllium Nickel Strip - Alloy 360 MH6, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Tensile Strength, Yield | >= 1034 MPa | >= 150000 psi | |
Materion Beryllium Nickel Strip - Alloy 360 Annealed, 2.5 hr at 950°F Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 2.5 hrs @ 510ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation.. |
|||
Tensile Strength, Yield | 1034 - 1340 MPa | 150000 - 194000 psi | |
Materion Beryllium Nickel Strip - Alloy 360 Hard Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 1.2Formability Ratio (bad Way).. |
|||
Tensile Strength, Yield | >= 1034 MPa @Strain 0.200 % |
>= 150000 psi @Strain 0.200 % |
|
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), >0.500-1.000 in, STD, Per Mil-T-9047G Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to >0.500-1.000 in, STD, Per Mil-T-9047G; other specific form/thickness entries are also available i.. |
|||
Tensile Strength, Yield | 1034 MPa @Strain 0.200 % |
150000 psi @Strain 0.200 % |
|
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 1150 AK Steel 17-4 PH® provides an outstanding combination of high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base.. |
|||
Tensile Strength, Yield | 1034 MPa @Strain 0.200 % |
150000 psi @Strain 0.200 % |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 25% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Tensile Strength, Yield | 1034 MPa @Strain 0.200 % |
150000 psi @Strain 0.200 % |
|
ATI Allvac® Vasco® Greek Ascoloy Specialty Steel, Heat Treatment: 871°C (1600°F) + Age Data provided by Allvac.Applications: Compressor blades, vanes, disks, shafts, wheels, fasteners, gas turbine and jet engine components. |
|||
Tensile Strength, Yield | 1034 MPa @Strain 0.200 % |
150000 psi @Strain 0.200 % |
|
Carpenter Custom 455® Stainless Steel, Annealed, 1.27 mm Strip Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |