Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 103 MPa | 14900 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ PS-30GF/15T Natural Polybutylene Terephthalate (PBT) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | F5, supporting material; ASTM D882 |
Rogers Corporation Poron® 4790-92-20 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | F5, supporting material; ASTM D882 |
Rogers Corporation Poron® 4790-92-30012 P Urethane Foam, Extra Soft, Slow Rebound, PET Film Reinforced Extra soft, slow rebound with a very low closure force. Available with thickness of 0.012" (0.30 mm).Features and Benefits of PORON Products: Excellent compression set resistance which enables dura.. |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | ASTM D638 |
Oxford Polymers 10GF 10% Glass Fiber Reinforced Polyetherimide/Polycarbonate Alloy 10% Glass Fiber Reinforced Polyetherimide/Polycarbonate AlloyInformation provided by Oxford Polymers. |
|||
Tensile Strength, Yield | 103 MPa | 14900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics EXTEM XH1015 TPI Resin (Europe-Africa-Middle East) Thermoplastic Polyimide Extem* XH1015 Resin. |
|||
Tensile Strength, Yield | 103 MPa | 14900 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® BFL2015HF PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only. UL94 V0 1.5 mm for BLACK; V1 1.5 mm for OTHER Color. |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | |
PSM Industries Pacific Sintered Metals Copper CU-143-W Powdered Metal High electrical and thermal conductivity, Good for heat sinks and electrical problemsInformation Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Yield | 103 MPa | 14900 psi | |
Reliance Industries PBT - 35% Glass filled Information provided by Reliance Industries |
|||
Tensile Strength, Yield | 103 MPa @Thickness 3.20 mm |
14900 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUMID LW4203A(W) PA6+GF/MF20%, Low Warpage Feature: Injection Molding, PA6+GF/MF20%, Low WarpageApplication: Automotive Parts (Engine Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
Tensile Strength, Yield | 103 MPa | 14900 psi | ASTM D638 |
Lucent Polymers LPB-130 Polybutylene Terephthalate, 30% Glass Fiber/Mineral Reinforced, Low Warp Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 103 MPa | 14900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 4001 PEI PTFE filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Tensile Strength, Yield | 103 MPa | 14900 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem DT1800E PEI Blend Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Americas re.. |
|||
Tensile Strength, Yield | 103 MPa | 14900 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem DT1800E PEI Blend (Europe-Africa-Middle East) Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Tensile Strength, Yield | 103 MPa | 14900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM EXUM0167 PEI Blend Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming. |
|||
Tensile Strength, Yield | 103 MPa | 14900 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem EXUM0169 PEI Blend (Europe-Africa-Middle East) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Tensile Strength, Yield | 103 MPa | 14900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® K4530 PBT (Europe-Africa-Middle East) 15% glass reinforced PBT, Hydrolytically stable, High flow, Automotive connectors. |
|||
Tensile Strength, Yield | 103 MPa | 14900 psi | Annealed |
Special Metals Nickel 201 Commercially pure (99.6%) wrought nickel essentially the same as Nickel 200 but with a lower carbon content to prevent embrittlement by intergranular carbon at temperatures over 600°F (315°C)... |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | ASTM D638 |
Techmer ES HiFill® TPX-HTN-01033 A 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthUL File .. |
|||
Tensile Strength, Yield | 103 MPa | 14900 psi | SABIC - Japan Method |
SABIC Innovative Plastics NORYL GTX CRN720V PPE+PA6 (Asia Pacific) GF20% FR-GTX, Restricted to sell for new customers |
|||
Tensile Strength, Yield | 103 - 317 MPa | 15000 - 46000 psi | 0.2% offset |
Eagle Brass 210 Gilding Metal, 1/4 Hard CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | ASTM D638 |
Clariant Renol PA143G10 Nylon 6/66 Copolymer, 10% Glass Fiber, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | >= 103 MPa @Strain 0.200 % |
>= 15000 psi @Strain 0.200 % |
|
Carlson 90 10 Cu Ni Copper-Nickel Alloy General DescriptionCarlson Alloy 90 10 Cu Ni is a copper-based alloy developed as a cost-effective substitute for 70 30 Cu Ni. An addition of approximately 1.4% iron was made to increase its resist.. |
|||
Tensile Strength, Yield | >= 103 MPa @Strain 0.200 % |
>= 15000 psi @Strain 0.200 % |
|
Carlson C 200 Commercially Pure Nickel General DescriptionCarlson Alloy C 200 is commercially pure nickel, combining good mechanical properties with excellent resistance to many corrosive environments. This alloy retains its strength at.. |
|||
Tensile Strength, Yield | 103 MPa | 14900 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® R220 Nylon 66, 40% mineral reinforced, DAM Vydyne® R220 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in natural, it is an injection-molding grade formulated to retain the inherent processing adva.. |
|||
Tensile Strength, Yield | 103 - 138 MPa @Strain 0.200 % |
14900 - 20000 psi @Strain 0.200 % |
|
Ametek High Purity Nickel Strip 899L Annealed Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Yield | 103 - 138 MPa @Strain 0.200 % |
14900 - 20000 psi @Strain 0.200 % |
|
Ametek High Purity Nickel Strip 899A Annealed Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | ASTM D638 |
Asahi Kasei Thermofil N3-13FG-1626 13% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 103 MPa | 14900 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DFP34 PC LNP* Lubricomp* DFP34 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | ASTM D638 |
Techmer ES HiFill® PA4/6 GF5 HS 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites, .. |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GFB20 20% Glass/Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead/Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat Stabiliz.. |