Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.90 MPa | 276 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® TPE 1502 Conductive Thermoplastic Compound PRE-ELEC® TPE 1502 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri.. |
|||
Tensile Strength, Yield | >= 1.90 MPa | >= 275 psi | Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 5723 Fluorocarbon-Elastomer Formulated Viton®. General service.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 1.90 MPa | 275 psi | AVG Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 7202 Nitrile Rubber Nitrile for oil & gas serviceInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 1.90 MPa | 275 psi | Transverse/Width |
Saint-Gobain Norton® Fluorglas® Chemfilm® R128/R129 Premium Grade Extruded Full Density PTFE Film (0.003" thick) Description: Full Density Unsintered Tape is used as primary insulation for high-temperature wires, jackets and cables and wall for convoluted hose. It meets the requirements of component insulation.. |
|||
Tensile Strength, Yield | 1.90 MPa | 276 psi | 508 mm/min; ASTM D638 |
Dow Engage® 8130 Polyolefin Elastomer Description: Engage® 8130 polyolefin elastomer is an ethyleneoctene copolymer with low density and a high melt index. This combination provides excellent toughness, flexibility, and ease in process.. |
|||
Tensile Strength, Yield | 1.90 MPa | 276 psi | 508 mm/min; ASTM D638 |
Dow Engage® 8150 Polyolefin Elastomer Description: Engage® 8150 and Engage® 8157 polyolefin elastomers are ethylene-octene copolymers that have excellent flow characteristics and provide good impact properties in blends with polypropy.. |
|||
Tensile Strength, Yield | 1.90 MPa | 276 psi | 508 mm/min; ASTM D638 |
Dow Engage® 8157 Polyolefin Elastomer Description: Engage® 8157 polyolefin elastomer is a loose talc surface coated ethylene-octene copolymer. The talc is untreated and has a nominal 1µm particle size. This product offers the exceptio.. |
|||
Tensile Strength, Yield | 1.90 MPa | 275 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® RT-3810M Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceDisclaimer.. |
|||
Tensile Strength, Yield | 1.90 MPa | 275 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® ST-6110 Thermoplastic Elastomer - SBC
(discontinued **) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |