Mechanical Properties Metric English Comments
Tensile Strength, Yield 1.00 MPa
145 psi
ASTM D638
Premix Thermoplastics PRESEAL® TPE 6080
General Description:PRESEAL® TPE 6080 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It can also be used as conductors or in grounding..
Tensile Strength, Yield 1.00 MPa
145 psi
ISO 37
Premix Thermoplastics PRESEAL® TPE 6080
General Description:PRESEAL® TPE 6080 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It can also be used as conductors or in grounding..
Tensile Strength, Yield 1.00 - 33.0 MPa
145 - 4790 psi
Average value: 12.5 MPa Grade Count:220
Overview of materials for Thermoplastic Olefinic Elastomer (TPO)
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v..
Tensile Strength, Yield 1.00 MPa
145 psi
At 100% elongation, across flow; ASTM D412
Advanced Elastomer Systems Santoprene® 8281-35W237 Thermoplastic Rubber  (discontinued **)
Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other ..
Tensile Strength, Yield 1.00 MPa
145 psi
ASTM D412
Polymax® Maxelast® C4902 TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Tensile Strength, Yield 1.00 MPa

@Strain 100 %
145 psi

@Strain 100 %
ASTM D412
Multibase Multi-Flex® D 4003 Black TPE Thermoplastic Elastomer
Forms: PelletsProcessing Methods:Injection MoldingExtrusion Information provided by Multibase
Tensile Strength, Yield >= 1.00 MPa
>= 145 psi
Stress at Elongation M100; ASTM D412 Method A
Seals Eastern 7017 Ethylene-Propylene Rubber
General service EPM.Information provided by Seals Eastern, Inc.
Tensile Strength, Yield 1.00 MPa
145 psi
AVG Stress at Elongation M25; ASTM D412 Method A
Seals Eastern 7282 Neoprene / Chloroprene
UL-flame resistant, non-blooming neopreneInformation provided by Seals Eastern, Inc.
Tensile Strength, Yield >= 1.00 MPa
>= 145 psi
Stress at Elongation M100; ASTM D412 Method A
Seals Eastern 7017 Ethylene-Propylene Rubber
General service EPM.Information provided by Seals Eastern, Inc.
Tensile Strength, Yield 1.00 MPa
145 psi
ACC MM810 Low Tear Condensation Cure 2-Part Molding Rubber
Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, good resistance to styrene attack, easy degassing, low shrinkage, range of catalysts. Applications: sh..
Tensile Strength, Yield 1.00 MPa
145 psi
ACC MM816 Low Tear Condensation Cure 2-Part Molding Rubber
Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, good resistance to styrene attack, easy degassing, low shrinkage, range of catalysts. Applications: sh..
Tensile Strength, Yield 1.00 MPa
145 psi
ACC MM820 Low Tear Condensation Cure 2-Part Molding Rubber
Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, good resistance to styrene attack, easy degassing, low shrinkage, range of catalysts. Applications: sh..
Tensile Strength, Yield 1.00 MPa
145 psi
ACC MM828 Low Tear Condensation Cure 2-Part Molding Rubber
Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, good resistance to styrene attack, easy degassing, low shrinkage, range of catalysts. Applications: sh..
Tensile Strength, Yield 1.00 - 18.9 MPa
145 - 2740 psi
Average value: 9.12 MPa Grade Count:41