Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 0.965 MPa | 140 psi | at 200%, post cured- 2 hours at 177°C |
Multibase SILASTIC® C7-4535 CADOX TS-50S Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 0.965 MPa | 140 psi | ISO 527-2 |
PolyOne Nymax™ GF 600 A 33 HS7 DX9 Black Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Tensile Strength, Yield | 0.965 MPa | 140 psi | at 200%, molded-without post cure; ASTM D412 |
Multibase C6-235 PERKADOX PD-50S Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 0.965 MPa | 140 psi | AVG Stress at Elongation M25; ASTM D412 Method A |
Seals Eastern 5862 Fluoro-silicone Fluoro-siliconeInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 0.965 MPa | 140 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® RT-3805M Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceDisclaimer.. |
|||
Tensile Strength, Yield | 0.965 MPa | 140 psi | at 100%; ASTM D412 |
R70-068 Styrene-based Biomedical Elastomer |
|||
Tensile Strength, Yield | 0.965 MPa | 140 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® ST-6105 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalOver-Molding GradeApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne Firs.. |