Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 0.600 MPa | 87.0 psi | ISO 37* |
Premix Thermoplastics PRESEAL® TPE 5010 PRESEAL TPE 5010 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It may also find interesting uses as conductors or in grounding applica.. |
|||
Tensile Strength, Yield | 0.600 MPa | 87.0 psi | 60°C for 1,000 hrs with 90% RH; JIS-K-6251(#2) |
Fujipoly Industries Sarcon® GR-c Gap Filler Pad Sarcon GR-c is a highly conformable, thermally conductive (no electric conductive) and electromagnetic wave absorption material in areas where space between surfaces is uneven and surface textures v.. |
|||
Tensile Strength, Yield | 0.600 MPa | 87.0 psi | 60°C for 1,000 hrs with 90% RH; JIS-K-6251(#2) |
Fujipoly Industries Sarcon® GR-Fd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Fd has a mesh embedded overall.Information provided b.. |
|||
Tensile Strength, Yield | 0.600 MPa | 87.0 psi | 150°C for 1,000 hrs; JIS-K-6251(#2) |
Fujipoly Industries Sarcon® GR-Hd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Hd has a hardened top surface.Information provided by.. |
|||
Tensile Strength, Yield | 0.600 MPa | 87.0 psi | 60°C for 1,000 hrs with 90% RH; JIS-K-6251(#2) |
Fujipoly Industries Sarcon® GR-Hd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Hd has a hardened top surface.Information provided by.. |
|||
Tensile Strength, Yield | 0.600 MPa | 87.0 psi | 70°C for 1,000 hrs; JIS-K-6251(#2) |
Fujipoly Industries Sarcon® GR-Hd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Hd has a hardened top surface.Information provided by.. |