Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 24.1 - 141 MPa | 3500 - 20500 psi | Average value: 55.9 MPa Grade Count:113 |
Overview of materials for High Density Polyethylene (HDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max.. |
|||
Film Tensile Strength at Break, MD | 26.2 - 141 MPa | 3800 - 20500 psi | Average value: 62.3 MPa Grade Count:15 |
Overview of materials for Polychlorotrifluoroethylene; Molded This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Film Tensile Strength at Break, MD | 75.8 - 141 MPa | 11000 - 20500 psi | ASTM D882 |
Honeywell ACLAR® 11A (0.90 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Film Tensile Strength at Break, MD | 97.9 - 141 MPa | 14200 - 20500 psi | ASTM D882 |
Honeywell Capran® K Coated Nylon Film
(discontinued **) Description: Capran® K is a PVdc coated nylon 6 film designed for food packaging applications where longer shelf life is required. This film exhibits good clarity, gloss, toughness, thermoformabil.. |
|||
Film Tensile Strength at Break, MD | 97.9 - 141 MPa | 14200 - 20500 psi | ASTM D882 |
Honeywell Capran® Nylon Film, Multipurpose Nylon 6 Film Description: Capran® is a multipurpose nylon 6 film. Its physical properties are evenly distributed for optimum performance giving excellent resistance to flex cracking. It can be processed ove.. |