Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 60.0 MPa | 8700 psi | Orientation not specified; ASTM D882 |
Nylene® 615 Nylon 6, Film Grade Film Grade. Nylene 615 is an extrusion grade nylon 6 resin suitable for coating and film co-extrusion applications. It has excellent melt stability and good melt strength. Nylene 615 has superior
.. |
|||
Film Tensile Strength at Break, MD | 60.0 MPa | 8700 psi | Orientation not specified; ASTM D882 |
Nylene® 615I Nylon 6, Film Grade Film Grade. Nylene 615I is an extrusion grade nylon 6 resin suitable for film co- extrusion applications and blown film. It has excellent melt stability and good melt strength. Nylene 615I has supe.. |
|||
Film Tensile Strength at Break, MD | 60.0 MPa | 8700 psi | Orientation not specified; ASTM D882 |
Nylene® 615SA Nylon 6, Film Grade Film Grade. Nylene 615SA is a Kosher, extrusion grade nylon 6 resin suitable for film co-extrusion applications and blown film. It has excellent melt stability and good melt strength. Nylene
615SA.. |
|||
Film Tensile Strength at Break, MD | 60.0 MPa | 8700 psi | Orientation not specified; ASTM D882 |
Nylene® NX3055I Nylon 6 Dry as molded. Film Grade. Nylene NX3055I is an extrusion grade nylon 6 suitable for cast film, blown film, and co-extrusion applications. NX3055I is highly crystalline which yields excellent roll.. |
|||
Film Tensile Strength at Break, MD | 60.0 MPa | 8700 psi | Orientation not specified; ASTM D882 |
Nylene® NX3411 Nylon 6 Film Grade. Nylene NX3411 is an extrusion grade nylon 6 resin suitable for film co-extrusion applications and blown film. It has excellent melt stability and good melt strength. Nylene NX3411 has
.. |
|||
Film Tensile Strength at Break, MD | 60.0 MPa | 8700 psi | ASTM D882 |
SABIC F00952 High Density Polyethylene for Blown Film Product Description: F00952 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Film Tensile Strength at Break, MD | 60.0 MPa | 8700 psi | ASTM D882 |
SABIC FJ00952 High Density Polyethylene for Blown Film Product Description: FJ00952 is a TNPP additive free, high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, .. |
|||
Film Tensile Strength at Break, MD | 60.0 MPa | 8700 psi | ASTM D882 |
Eastman 9921P PET Film
(discontinued **) Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia.. |
|||
Film Tensile Strength at Break, MD | 60.0 MPa | 8700 psi | ASTM D882 |
ExxonMobil Exceed™ 377D60 LDPE/Hexene Tough Premium Film Resin, 0.8 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 377D60 resin exhibit excellent impact strength and b.. |
|||
Film Tensile Strength at Break, MD | 60.0 MPa | 8700 psi | ISO 527-3 |
Total PPH 6088 Polypropylene Homopolymer, Cast Film Polypropylene PPH 6088 is a homopolymer polypropylene with a Melt Flow index of 9 g/10 min for the cast extrusion of film with excellent optical properties and good sterilizability.Polypropylene PPH.. |
|||
Film Tensile Strength at Break, MD | 60.0 MPa | 8700 psi | ASTM D882 |
Formosa Plastics Formolene® E924ND Film HDPE High Molecular Weight High Density Polyethylene (HMW-HDPE) for Film Extrusion Formolene® E924ND is a bi-modal HMW-HDPE resin designed for high dart impact strength and good processing characteristi.. |
|||
Film Tensile Strength at Break, MD | 60.0 MPa | 8700 psi | ASTM D882 |
ExxonMobil Enable™ 20-05HE Metallocene Polyethylene Resin Product Description: Enable 20-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Film Tensile Strength at Break, MD | 60.0 MPa | 8700 psi | ASTM D882 |
ExxonMobil Enable™ 20-05HH Metallocene Polyethylene Resin (Asia Pacific Grade) Product Description: Enable 20-05 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Film Tensile Strength at Break, MD | 60.0 MPa | 8700 psi | ASTM D882 |
ExxonMobil Enable™ 20-05HH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 20-05HH is a metallocene ethylene-hexene copolymer. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and p.. |
|||
Film Tensile Strength at Break, MD | 60.0 MPa | 8700 psi | ASTM D882 |
ExxonMobil Exceed™ 2018HA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2018HA is a metallocene Catalyzed ethylene-hexene copolymer. Films made from Exceed 2018HA have outstanding tensile, impact strength, and puncture. These superior strengt.. |
|||
Film Tensile Strength at Break, MD | 60.0 MPa | 8700 psi | ASTM D882 |
ExxonMobil LLDPE LL 1201KG Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 1201 series are LLDPE grades, offering excellent combination of stiffness and optical properties (when blended with 10-20% LDPE) Availability: Africa & Middle East, Asia Paci.. |
|||
Film Tensile Strength at Break, MD | 60.0 MPa | 8700 psi | ASTM D882 |
ExxonMobil LLDPE LL 1201XV Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 1201 series are LLDPE grades, offering excellent combination of stiffness and optical properties (when blended with 10-20% LDPE) Availability: Africa & Middle East, Asia Paci.. |
|||
Film Tensile Strength at Break, MD | 60.0 MPa @Thickness 0.0150 mm |
8700 psi @Thickness 0.000591 in |
ASTM D882 |
Equate EGDA-6888 HDPE Film Extrusion Resin EGDA-6888 is a high molecular weight, high density polyethylene copolymer that has been designed specifically for tubular film extrusion. Its broad molecular weight distribution and density have bee.. |
|||
Film Tensile Strength at Break, MD | 60.0 MPa | 8700 psi | |
Dow DOWLEX™ NG 3347A Linear Low Density Polyethylene, Ethylene-Octene Copolymer Next Generation DOWLEX® NG 3347A resin with extra stretch performance (ESP)is an ethylene-octene-1 copolymer designed for cast stretch film applications such as industrial pallet wrap. DOWLEX NG 33.. |
|||
Film Tensile Strength at Break, MD | 60.0 MPa | 8700 psi | ASTM D882 |
ExxonMobil Enable™ 20-05HE Metallocene Polyethylene Resin (Asia Pacific Grade) Product Description: Enable 20-05 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Film Tensile Strength at Break, MD | 60.0 MPa | 8700 psi | ASTM D882 |
ExxonMobil Enable™ 20-05HH Metallocene Polyethylene Resin Product Description: Enable 20-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Film Tensile Strength at Break, MD | 60.0 MPa | 8700 psi | ASTM D882 |
ExxonMobil Enable™ 20-05CB Metallocene Polyethylene Resin Product Description: Enable 20-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Film Tensile Strength at Break, MD | 60.0 MPa | 8700 psi | ASTM D882 |
ExxonMobil Enable™ 35-05CH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 35-05CH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |
|||
Film Tensile Strength at Break, MD | 60.0 MPa | 8700 psi | ASTM D882 |
Braskem HF 0144 HDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags. Information provided by Bras.. |
|||
Film Tensile Strength at Break, MD | 60.0 MPa | 8700 psi | cast films; ISO 527-3 |
Borealis Bormod™ HC904CF Polypropylene Bormod™ BJ368MO is a polypropylene copolymer characterized by good flow, and optimum combination of high stiffness and high impact strength. The material is nucleated with Borstar® Nucleation Tech.. |