Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 59.0 MPa | 8560 psi | ASTM D882 |
Eastman EASTALLOY Polymer DA003-8999K, Clear Alloy
(discontinued **) Properties below based on a film thickness of 250 microns. CO2 Permeability is 49 cm3·mm/m2·24h·atm per ASTM D 1434.Product Description: EASTALLOY DA003-8999K Polymer is a clear copolyester/pol.. |
|||
Film Tensile Strength at Break, MD | 59.0 MPa | 8560 psi | Orientation not specified; ASTM D882 |
EVALCA EVAL® LC-H101BD Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 38 mol % Ethylene.Data provided by EVALCA. Applications: Blown film. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of th.. |
|||
Film Tensile Strength at Break, MD | 59.0 MPa | 8560 psi | ISO 527-3 |
Total Lumicene® mPE M 2310 EP Metallocene Polyethylene, Blown Film Lumicene® mPE M 2310 EP is a second generation metallocene based Linear Low Density Polyethylene with hexene as comonomer.Lumicene® mPE M 2310 EP can be processed at high output rates with low ext.. |
|||
Film Tensile Strength at Break, MD | 59.0 MPa | 8560 psi | ASTM D882 |
Eastman Eastman 1223 Copolyester Applications:Blown filmCredit cardsDebit cardsDeodorant packagingElectronic packagingFabricated boxesFlexible packagingFood packagingFurniture/Furniture trimGaming cardsGift cardsIdentification card.. |
|||
Film Tensile Strength at Break, MD | 59.0 MPa | 8560 psi | ASTM D882 |
Eastman GSP01 Copolyester for Film and Sheet Extrusion Applications:Consumer e-packaging trayElectronic packagingElectrostatic dissipative trayProduct Description: GSP01 is a clear, amorphous material. Because of its clarity, toughness and good melt s.. |
|||
Film Tensile Strength at Break, MD | 59.0 MPa | 8560 psi | ASTM D882 |
Eastman Tritan FX100 Copolyester Eastman Tritan FX100 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w.. |
|||
Film Tensile Strength at Break, MD | 59.0 MPa | 8560 psi | ASTM D882 |
Eastman Tritan MP100 Copolyester Eastman Tritan MP100 is an amorphous copolyester that combines excellent clarity and toughness with outstanding heat and chemical resistance. Film and sheet manufactured from this new-generation co.. |
|||
Film Tensile Strength at Break, MD | 59.0 MPa | 8560 psi | Blown Film at 1 mil; ASTM D-882 |
Chevron Phillips MarFlex® 7105D Polyethylene; LLDPE Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: High strengthGood drawdownGood processabilityUse alone or in blends with LDPE or HDPE Appl.. |
|||
Film Tensile Strength at Break, MD | 59.0 MPa | 8560 psi | ASTM D882 |
Chevron Phillips MarFlex® D139DK Metallocene Linear Low Density Polyethylene, Blown Film This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du.. |
|||
Film Tensile Strength at Break, MD | 59.0 MPa | 8560 psi | ASTM D882 |
Chevron Phillips MarFlex® D139FK Metallocene Linear Low Density Polyethylene, Blown Film This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du.. |
|||
Film Tensile Strength at Break, MD | 59.0 MPa | 8560 psi | ASTM D882 |
Westlake Hifor LT74107-F Polyethylene Film, Using Energx Technology Services
(discontinued **) Hifor LT74107-F polymer is a high strength and good clarity polyethylene designed for blown film extrusion that contains medium slip, high antiblock and high processing aid additives. Films produced.. |