Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 53.9 MPa | 7820 psi | ASTM D882 |
Lotte Chemical Titan TITANCEED® mL1061 Linear low density polyethylene resin
(discontinued **) Titanceed® mL1061 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant, antiblock and slip agent. Films made from Titanceed® mL1061 have outstanding tensile.. |
|||
Film Tensile Strength at Break, MD | 53.9 MPa | 7820 psi | ASTM D882 |
Lotte Chemical Titan TITANCEED® mL1064 Linear low density polyethylene resin
(discontinued **) Titanceed® mL1064 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. Films made from Titanceed® mL1064 have outstanding tensile, impact and puncture stre.. |
|||
Film Tensile Strength at Break, MD | 53.9 MPa | 7820 psi | ASTM D882 |
Lotte Chemical Titan TITANCEED® mL156 Linear low density polyethylene resin
(discontinued **) Titanceed® mL156 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding tensile strengt.. |
|||
Film Tensile Strength at Break, MD | 53.9 MPa | 7820 psi | ASTM D882 |
Lotte Chemical Titan TITANCEED® mL216 Linear low density polyethylene resin
(discontinued **) Titanceed® mL216 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding tensile strengt.. |
|||
Film Tensile Strength at Break, MD | 53.9 MPa | 7820 psi | ASTM D882 |
Lotte Chemical Titan TITANEX® HF1881 High density polyethylene Hexene-1 resin HF1881 is a pelleted medium molecular weight, high density polyethylene Hexene-1 resin for tubular film extrusion.Applications: Grocery sacks, shopping bags, liners and thin films.Advantages: Speci.. |
|||
Film Tensile Strength at Break, MD | 53.9 MPa | 7820 psi | |
Dow Elite® 5400 Linear Low Density Polyethylene 5400 enhanced polyethylene resin is a copolymer produced via INSITE technology from Dow Plastics. It offers extremely high impact resistance, combined with excellent tear, tensile, and optical prop.. |