Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 44.8 MPa | 6500 psi | ASTM D882 |
LyondellBasell Petrothene® LP540200 High Density Polyethylene ApplicationsPETROTHENE LP 5402-00 is a copolymer resin designed for blown film applications. This resin offers high stiffness, excellent appearance and bubble stability and good draw-down. LP 5402-0.. |
|||
Film Tensile Strength at Break, MD | 44.8 MPa | 6500 psi | ASTM D882 |
Westlake LF2010 Hexene Linear Low Density Polyethylene Westlake LF2010 is a hexene LLDPE with increased stiffness suitable for heavy duty films and shipping sacks. This material contains process aid for improved ease of extrusion, and can be blended wit.. |
|||
Film Tensile Strength at Break, MD | 44.82 MPa | 6500 psi | ASTM D882 |
Formosa Plastics Formolene® L62022B Film (Hexene Grade) LLDPE Hexene Copolymer (Barefoot)Applications: Cast stretch film and high quality packaging films requiring clarity and toughness.A Hexene Copolymer Linear Low Density Polyethylene for film applications i.. |
|||
Film Tensile Strength at Break, MD | 44.82 MPa | 6500 psi | ASTM D882 |
Formosa Plastics Formolene® L62030B Film (Hexene Grade) LLDPE Hexene Copolymer (Barefoot)Applications: Cast stretch film and high quality packaging films requiring clarity and toughness.A Hexene Copolymer Linear Low Density Polyethylene for film applications i.. |
|||
Film Tensile Strength at Break, MD | 44.8 MPa | 6500 psi | ASTM D882 |
ExxonMobil LLDPE LL 1236.85 Linear Low Density Polyethylene Resin Product Description: LL 1236 Series resins are butane LLDPEs with increased stiffness and a high melt index. They can be used alone or as a component in packaging and industrial film, blown or cast... |
|||
Film Tensile Strength at Break, MD | 44.8 MPa | 6500 psi | ASTM D882 |
ExxonMobil LLDPE LL 1236.86 Linear Low Density Polyethylene Resin Product Description: LL 1236 Series resins are butane LLDPEs with increased stiffness and a high melt index. They can be used alone or as a component in packaging and industrial film, blown or cast... |
|||
Film Tensile Strength at Break, MD | 44.8 MPa | 6500 psi | |
Dow DOWLEX™ 2045.02AC Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2045.02AC Polyethylene resin is a high stability blown film extrusion resin that provides excellent tear strength and outstanding toughness. It contains high level of slip additive and medi.. |
|||
Film Tensile Strength at Break, MD | 44.8 MPa | 6500 psi | ASTM D882 |
M. Holland Company MAGMA® LM203-C LLDPE
(discontinued **) Features: Good Heat Seal, Good Tear Strength, Good ToughnessUses: BlendingProcessing Method: ExtrusionInformation provided by M. Holland. |