Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 33.7 MPa | 4890 psi | MD-TD Average; ASTM D882 |
DuPont Elvax® 3129 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
(discontinued **) 10 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra.. |