Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 31.7 MPa | 4600 psi | 50 µm (2 mil) film; ASTM D882 |
DuPont Nucrel® 903 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 9 wt% Methacrylic Acid.Nucrel® 0903 is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process pol.. |
|||
Film Tensile Strength at Break, MD | 31.7 MPa | 4600 psi | ASTM D882 |
ExxonMobil Escorene™ FL 00018 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00018 is a copolymer of ethylene and vinyl acetate. It offers combines toughness, good optical and sealing properties and low gel. In particular, its good behavior in high fr.. |
|||
Film Tensile Strength at Break, MD | 31.7 MPa | 4600 psi | ASTM D882 |
ExxonMobil Escorene™ UL 00018 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00018 is a fractional MI copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applic.. |
|||
Film Tensile Strength at Break, MD | 31.7 MPa | 4600 psi | ASTM D882 |
Amco PRIMATOP LLDPE 009919B Linear Low Density Polyethylene, Butene Copolymer for Film LLDPE 009919B features excellent toughness and strength when drawn down to thin gauges. Applications include blending resin, industrial packaging, coextrusion, industrial liners, and garment bags.Fo.. |