Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 24.3 MPa | 3530 psi | ASTM D882 |
ExxonMobil LD 334.57 Clear, High Impact Film Resin LD 334 resins produce films with superior impact strength, good heat sealability, and low temperature properties.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Break, MD | 24.3 MPa | 3530 psi | ASTM D882 |
ExxonMobil LD 334.82 Clear, High Impact Film Resin LD 334 resins produce films with superior impact strength, good heat sealability, and low temperature properties.Information provided by ExxonMobil Chemical |