Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 21.0 MPa | 3050 psi | ISO 527-3 |
Polimeri Europa Riblene® FM 50 Low Density Polyethylene - Blown Film Extrusion Riblene FM 50 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FM 50 is characterized by optimum optical properties and rigidity.Films manufactured with Riblene FM 50.. |
|||
Film Tensile Strength at Break, MD | 21.0 MPa | 3050 psi | ISO 527-3 |
Polimeri Europa Riblene® FM 53 Low Density Polyethylene - Blown Film Extrusion Riblene FM 53 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FM 53 is characterized by optimum optical properties and rigid.. |
|||
Film Tensile Strength at Break, MD | 21.0 MPa | 3050 psi | ASTM D882 |
Petroquimica Triunfo Trithene® CX 7020 LDPE - Cast Film The Trithene® CX 7020 resin is a low-density polyethylene (LDPE) with medium molecular weight, excellent processability, and low gel content. Those features allow a production of thin and highly un.. |
|||
Film Tensile Strength at Break, MD | 21.0 MPa | 3050 psi | ASTM D882 |
Eastman D4028-F Polyethylene
(discontinued **) D4028-F is a low density formulation which contains high antiblock. It is suggested for film applications that require reasonable clarity. D4028-F meets the requirements of FDA regulations at 21 CF.. |
|||
Film Tensile Strength at Break, MD | 21.0 MPa | 3050 psi | ASTM D882 |
Eastman E6838-014F Polyethylene
(discontinued **) E6838-014F is a low density formulation that contains low slip and medium antiblock levels. It is suggested for film applications that require clarity.List of Applications: Food packagingFood-conta.. |
|||
Film Tensile Strength at Break, MD | 21.0 MPa | 3050 psi | Non-oriented film; ASTM D882 |
Total PPR 8573 Polypropylene, Film Extrusion Grade Random copolymer heat sealable film gradeColor/Clarity/Impact - FINA 8573 is a low melting, high ethylene random copolymer with improved color, optics and impact properties.Heat Sealable - The low m.. |
|||
Film Tensile Strength at Break, MD | 21.0 - 56.5 MPa | 3050 - 8200 psi | Average value: 38.7 MPa Grade Count:23 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi.. |
|||
Film Tensile Strength at Break, MD | 21.0 MPa | 3050 psi | |
Reliance Industries LLDPE film - Active alumina + zeolite based film Information provided by Reliance Industries |
|||
Film Tensile Strength at Break, MD | 21.0 MPa | 3050 psi | ASTM D882 |
ExxonMobil Escorene® LD-734 High EVA Extrusion Coating Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate extrusion coating resin which provides outstanding heat sealability and high clarity. It has a good balance of drawability and.. |
|||
Film Tensile Strength at Break, MD | 21.0 MPa | 3050 psi | ASTM D882 |
SABIC HP2022 Series Low Density Polyethylene for Blown Film Product Description: HP2022 series resins are Low Density Polyethylene grades suitable for general purpose packaging. They exhibit better draw down, good optical and mechanical properties.HP2022N:.. |