Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 13.0 MPa | 1890 psi | ISO 527-3 |
Polimeri Europa Clearflex® CH G0 Very Low Density Polyethylene Clearflex CH G0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin has an excellent compatibility with polyolefins and fillers.Main Applic.. |
|||
Film Tensile Strength at Break, MD | 13.0 MPa | 1890 psi | ASTM D3759 |
3M Scotch® 355 Superior Performance Box Sealing Tape Scotch® Box Sealing Tape 355 is a superior performance packaging tape used for box sealing, splicing, recouperage and other demanding packaging applications. This product has a strong abrasion resi.. |
|||
Film Tensile Strength at Break, MD | 13.0 - 76.6 MPa | 1890 - 11100 psi | Average value: 46.6 MPa Grade Count:12 |
Overview of materials for Very Low Density Polyethylene (VLDPE) This property data is a summary of similar materials in the MatWeb database for the category "Very Low Density Polyethylene (VLDPE)". Each property range of values reported is minimum and maximum va.. |