Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 8.45 MPa | 1230 psi | ASTM D3759 |
3M Scotch® 600 Transparent Film Tape Scotch® Tape 600 is a transparent film tape that is excellent for various packaging applications. It has a pressure sensitive acrylic adhesive system which is long aging and highly transparent, so .. |