Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 82.0 MPa | 11900 psi | parallel; ISO 527-3 |
DSM Akulon® F130 PA6 Film Extrusion, Medium Viscosity |
|||
Film Tensile Strength at Break, MD | 82.0 MPa | 11900 psi | parallel; ISO 527-3 |
DSM Akulon® F130-C PA6 Film Extrusion, Medium Viscosity, Lubricated |
|||
Film Tensile Strength at Break, MD | 82.0 MPa | 11900 psi | parallel; ISO 527-3 |
DSM Akulon® F130-C2 PA6 Medium Viscosity, Film Extrusion, Lubricated |
|||
Film Tensile Strength at Break, MD | 82.0 MPa | 11900 psi | parallel; ISO 527-3 |
DSM Akulon® F130-C3 PA6 Monofilament Grade, Extrusion Grade, Medium Viscosity, Lubricated |