Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 24.0 - 41.0 MPa | 3480 - 5950 psi | Average value: 32.0 MPa Grade Count:17 |
Overview of materials for Ionomer, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |