Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 290 - 359 MPa | 42000 - 52000 psi | ASTM D882 |
Honeywell Capran® Unidraw (1.00 mil) Nylon 6 Film
(discontinued **) Description: Capran® Unidraw is a 1.00 mil (25 micron) machine direction oriented nylon 6 film specifically designed for the continuous process lamination of glass fiber reinforced panel. High str.. |