Polymer Property : Film Tensile Strength at Break, MD = 141 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 24.1 - 141 MPa
3500 - 20500 psi
Average value: 55.9 MPa Grade Count:113
Overview of materials for High Density Polyethylene (HDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max..
Film Tensile Strength at Break, MD 26.2 - 141 MPa
3800 - 20500 psi
Average value: 62.3 MPa Grade Count:15
Overview of materials for Polychlorotrifluoroethylene; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu..
Film Tensile Strength at Break, MD 75.8 - 141 MPa
11000 - 20500 psi
ASTM D882
Honeywell ACLAR® 11A (0.90 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.
Film Tensile Strength at Break, MD 97.9 - 141 MPa
14200 - 20500 psi
ASTM D882
Honeywell Capran® K Coated Nylon Film  (discontinued **)
Description: Capran® K is a PVdc coated nylon 6 film designed for food packaging applications where longer shelf life is required. This film exhibits good clarity, gloss, toughness, thermoformabil..
Film Tensile Strength at Break, MD 97.9 - 141 MPa
14200 - 20500 psi
ASTM D882
Honeywell Capran® Nylon Film, Multipurpose Nylon 6 Film
Description: Capran® is a multipurpose nylon 6 film. Its physical properties are evenly distributed for optimum performance giving excellent resistance to flex cracking. It can be processed ove..