Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 44.6 MPa | 6470 psi | Calculated from mfr's report of 229 N/cm per ASTM D828 and the typical thickness |
DuPont™ Nomex® E56 Paper, 20 mil Nominal Thickness Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as.. |
|||
Film Tensile Strength at Break, MD | 44.6 MPa | 6470 psi | ASTM D882 |
Dow AFFINITY™ PL 1850G Polyolefin Plastomer (POP) AFFINITY™ PL 1840G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed to provide blown and cast film products with low temperature sealability, excellent optics and g.. |