Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 33.8 MPa | 4900 psi | ASTM D882 |
LyondellBasell Petrothene® GA502022 Linear Low Density Polyethylene ApplicationsThe PETROTHENE GA 502 series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These pelletized produc.. |
|||
Film Tensile Strength at Break, MD | 33.8 MPa | 4900 psi | ASTM D882 |
LyondellBasell Petrothene® GA502024 Linear Low Density Polyethylene ApplicationsThe PETROTHENE GA 502 series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These pelletized produc.. |
|||
Film Tensile Strength at Break, MD | 33.8 MPa | 4900 psi | ASTM D882 |
LyondellBasell Petrothene® GA502023 Linear Low Density Polyethylene ApplicationsThe PETROTHENE GA 502 series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These pelletized produc.. |
|||
Film Tensile Strength at Break, MD | 33.8 MPa | 4900 psi | ASTM D882 |
Westlake EN1817AA Low Density Polyethylene Westlake Polyethylene EN1817 is a low density formulation suggested for film applications requiring high clarity, good tear and impact strength, good printability and a wide heat-sealing range.Appli.. |
|||
Film Tensile Strength at Break, MD | 33.8 MPa | 4900 psi | ASTM D882 |
Westlake EN1820 Low Density Polyethylene Westlake Polyethylene EN1820 natural is a low density formulation with outstanding optical properties, making this material an excellent choice for calendaring and as a clarity filler in coextruded .. |
|||
Film Tensile Strength at Break, MD | 33.8 MPa | 4900 psi | ASTM D882, A |
Total Lumicene® mPE M 2710 EP Metallocene Polyethylene, Film Metallocene Medium Density Film ResinCharacteristics:Outstanding clarity and glossExcellent bubble stabilityExcellent tear strengthHigh puncture resistanceGood stiffnessExcellent heat sealing proper.. |
|||
Film Tensile Strength at Break, MD | 33.8 MPa @Thickness 0.0254 mm |
4900 psi @Thickness 0.00100 in |
ASTM D882A |
Total Lumicene® mPE M 3410 EP HDPE Film Outstanding clarity and gloss; excellent bubble stability; excellent tear strength; high puncture resistance; good stiffness; excellent heat sealing properties; excellent compatibility with LDPE and.. |
|||
Film Tensile Strength at Break, MD | 33.8 MPa | 4900 psi | ASTM D882 |
ExxonMobil Escorene™ FL 00014 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00014 is a copolymer of ethylene and vinyl acetate. For film requiring very high toughness, low creep, excellent optical properties and low gel.Availability: Africa & Middle .. |
|||
Film Tensile Strength at Break, MD | 33.8 MPa | 4900 psi | ASTM D882 |
ExxonMobil Escorene™ UL 00014 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00014 is a fractional MI copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applic.. |
|||
Film Tensile Strength at Break, MD | 33.8 MPa | 4900 psi | ASTM D882 |
DuPont™ Surlyn® 1601 Sodium Ionomer Resin for Blown and Cast Film Surlyn® 1601 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea.. |
|||
Film Tensile Strength at Break, MD | 33.8 MPa | 4900 psi | ASTM D882 |
DuPont™ Surlyn® 1601-2 Sodium Ionomer Resin for Blown and Cast Film Surlyn® 1601-2 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, s.. |
|||
Film Tensile Strength at Break, MD | 33.8 MPa | 4900 psi | ASTM D882 |
DuPont™ Surlyn® 1601-2LM Sodium Ionomer Resin for Blown and Cast Film Surlyn® 1601-2LM (Low Moisture) is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications:.. |
|||
Film Tensile Strength at Break, MD | 33.8 MPa | 4900 psi | ASTM D882 |
DuPont™ Surlyn® 1650 Zinc Ionomer Resin for Blown and Cast Film Surlyn® 1650 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea.. |