Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 29.6 MPa | 4300 psi | ASTM D882 |
Chevron Phillips MarFlex® 7109L LLDPE Blown Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Film Tensile Strength at Break, MD | 29.6 MPa | 4300 psi | ASTM D882 |
M. Holland Company LL102 LLDPE
(discontinued **) Additives: Medium Antiblock, Medium SlipFeatures: Medium Antiblocking, Butene Comonomer, Copolymer, Good Drawdown, Good Processability, Medium SlipUses: Film, LinersApprovals: FDA 21 CFR 177.1520(c).. |
|||
Film Tensile Strength at Break, MD | 29.6 MPa | 4290 psi | ASTM D882 |
DuPont™ Surlyn® 1601B Sodium Ionomer Resin for Blown and Cast Film
(discontinued **) Surlyn® 1601B is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, se.. |
|||
Film Tensile Strength at Break, MD | 29.6 MPa | 4300 psi | ASTM D882 |
Westlake Hifor Xtreme SC74840 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74840 linear low density polyethylene is recommended for the core layer of cast stretch film. It provides excellent clarity and ultimate stretch values higher than the more c.. |
|||
Film Tensile Strength at Break, MD | 29.6 MPa | 4300 psi | ASTM D882 |
Westlake Mxsite LC78104 Polyethylene Mxsite LC78104 polyethylene is recommended for the skin layers of cast stretch film. It will provide a very aggressive cling force in both a stretched and unstretched condition. The excellent cling .. |
|||
Film Tensile Strength at Break, MD | 29.6 MPa | 4300 psi | ASTM D882 |
Chevron Phillips MarFlex® 7109DL LLDPE Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Film Tensile Strength at Break, MD | 29.6 MPa | 4300 psi | ASTM D882 |
Chevron Phillips MarFlex® 7109M LLDPE Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Film Tensile Strength at Break, MD | 29.6 MPa | 4290 psi | |
Dow AFFINITY™ HF 1030 Polyolefin Plastomer AFFINITY® HF 1030 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide cast embossed film products with high modulus for machinability, excellent drawdown at high line speeds,.. |
|||
Film Tensile Strength at Break, MD | 29.6 MPa | 4290 psi | |
Dow LDPE 640I Low Density Polyethylene, Liner Film Grade DOW LDPE 640I resin is a barefoot general purpose liner film resin for thin gauge applications requiring good drawdown and excellent toughness. This material complies with U.S.FDA regulation 21 CFR .. |
|||
Film Tensile Strength at Break, MD | 29.6 MPa | 4300 psi | ASTM D882 |
ExxonMobil Escorene™ LD 708.62 Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 708.62 is a 14.9% VA copolymer film resin. Film made from LD 708.62 exhibits good impact strength and superior heat sealabilty.Availability: Latin America, Nor.. |
|||
Film Tensile Strength at Break, MD | 29.6 MPa | 4300 psi | ASTM D882 |
M. Holland Company LL106 LLDPE
(discontinued **) Additives: Antiblock, SlipFeatures: Unspecified Antiblocking, Hexane Comonomer, Copolymer, Good Drawdown, Good Processability, Unspecified SlipUses: Film, LinersApprovals: FDA 21 CFR 177.1520(c) 2.2.. |
|||
Film Tensile Strength at Break, MD | 29.6 MPa | 4290 psi | ASTM D882 |
DuPont™ Surlyn® 1601B-2 Sodium Ionomer Resin for Blown and Cast Film
(discontinued **) Surlyn® 1601 B-2 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry,.. |
|||
Film Tensile Strength at Break, MD | 29.6 MPa | 4300 psi | ASTM D882 |
Chevron Phillips MarFlex® 7109CL LLDPE Blown Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |