Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 23.4 MPa | 3400 psi | ASTM D882 |
LyondellBasell Petrothene® M2520FN Low Density Polyethylene ApplicationsPETROTHENE M 2520 is a film grade resin that exhibits excellent optics, good gloss and good bubble stability. A typical application for this resin is high clarity packaging. Regulatory.. |
|||
Film Tensile Strength at Break, MD | 23.4 MPa | 3400 psi | ASTM D882 |
LyondellBasell Petrothene® NA143063 Low Density Polyethylene ApplicationsPETROTHENE NA 143 is a series of homopolymer resins for blown film. Applications include stiff liners. Regulatory StatusNA 143 meets the requirements of the Food and Drug Administration.. |
|||
Film Tensile Strength at Break, MD | 23.4 MPa | 3400 psi | ASTM D882 |
LyondellBasell Petrothene® NA963083 Low Density Polyethylene ApplicationsPETROTHENE NA 963 is a series of resins formulated with special antiblock additive and designed for a wide variety of industrial film applications where high impact strength and excellen.. |
|||
Film Tensile Strength at Break, MD | 23.4 MPa | 3400 psi | ASTM D882 |
Westlake EP310 Low Density Polyethylene WESTLAKE polyethylene EP310 is a low-density polyethylene suggested for cast film bakery applications. This material has outstanding optical and processing properties.Application/UsesBakery bagsSoft.. |
|||
Film Tensile Strength at Break, MD | 23.4 MPa | 3400 psi | ASTM D882 |
ExxonMobil LDPE LD 129.24 Low Density Polyethylene Resin Product Description: LD 129.24 is a medium density homopolymer film resin with good clarity and excellent stiffness. Film made from LD 129.24 can be used in overwrap applications and in push-through.. |
|||
Film Tensile Strength at Break, MD | 23.4 MPa | 3400 psi | ASTM D882 |
ExxonMobil Optema® TC-110 Cast Ethylene Methyl Acrylate Product Description: Optema TC 110 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown and cast film applications. It can produce f.. |
|||
Film Tensile Strength at Break, MD | 23.4 MPa | 3400 psi | ASTM D882 |
Dow INTEGRAL™ 900 Deep Draw Multilayer Adhesive Film INTEGRAL 900 Adhesive Film is a heat-activated, moldable, thermally stable adhesive film capable of bonding to urethane foam-baked fabrics, polyester and nylon fabrics, fiberglass, and rigid urethan.. |
|||
Film Tensile Strength at Break, MD | 23.4 MPa | 3390 psi | |
Dow LDPE 133A Low Density Polyethylene, Blown Film Grade DOW LDPE 133A resin is used for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It contains medium levels of antib.. |
|||
Film Tensile Strength at Break, MD | 23.4 MPa | 3390 psi | |
Dow LDPE 135A Low Density Polyethylene, Blown Film Grade DOW LDPE 135A resin is used for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It contains medium levels of slip .. |
|||
Film Tensile Strength at Break, MD | 23.4 MPa | 3390 psi | |
Dow LDPE 170A Low Density Polyethylene, Blown Film Grade DOW LDPE 170A resin is used for shrink and heavy duty blown film applications where optical clarity is desired. It contains medium level of antiblock additives. It complies with U.S. FDA regulation .. |
|||
Film Tensile Strength at Break, MD | 23.4 MPa | 3390 psi | |
Dow LDPE 132I Low Density Polyethylene, Blown Film Grade DOW LDPE 132I is a barefoot resin for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It complies with U.S. FDA re.. |
|||
Film Tensile Strength at Break, MD | 23.4 MPa | 3400 psi | ASTM D882 |
Dow XU 66129.00 Developmental Monolayer Adhesive Film XU 66129.00 Developmental Monolayer Adhesive Film is a heat-activated, thermally stable adhesive film capable of bonding to urethane foam-backed fabrics, paper, fiberglass, non-wovens, and rigid ure.. |