Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 22.8 MPa | 3300 psi | ASTM D882 |
LyondellBasell Petrothene® NA420127 Low Density Polyethylene
(discontinued **) ApplicationsPETROTHENE NA 420 is a LDPE/EVA copolymer resin for high impact and clarity packaging film. This resin exhibits excellent processability over a broad range of extrusion conditions. Wel.. |
|||
Film Tensile Strength at Break, MD | 22.8 MPa | 3300 psi | ASTM D882 |
M. Holland Company EV200 EVA
(discontinued **) Features: Good Heat Seal, Opticals, High StrengthUses: PackagingApprovals: FDA 21 CFR 177.1350 and FDA 21 CFR 176.170,Table 2, Cond. C, D, E, F, GProcessing Method: Film, BlownInformation provided b.. |
|||
Film Tensile Strength at Break, MD | 22.8 MPa | 3300 psi | ASTM D882 |
LyondellBasell Petrothene® NA420000 Low Density Polyethylene ApplicationsPETROTHENE NA 420 is a LDPE/EVA copolymer resin for high impact and clarity packaging film. This resin exhibits excellent processability over a broad range of extrusion conditions. Wel.. |
|||
Film Tensile Strength at Break, MD | 22.8 MPa | 3300 psi | ASTM D882 |
LyondellBasell Petrothene® NA426225 Low Density Polyethylene, Film Extrusion Grade PETROTHENE NA426 is a series of LDPE/EVA copolymer resins for high impact and clarity packaging film. These resins exhibit excellent a broad range of extrusion conditions. Well-balanced films with e.. |
|||
Film Tensile Strength at Break, MD | 22.8 MPa | 3300 psi | ASTM D882 |
Westlake Elevate™ EF545 4% Ethylene Vinyl Acetate Copolymer Westlake EF545 resin is a 4% EVA copolymer designed for films that require excellent optical and strength properties. This Kosher compliant resin has excellent heat sealing characteristics and low t.. |
|||
Film Tensile Strength at Break, MD | 22.8 MPa | 3300 psi | ASTM D882 |
ExxonMobil LDPE LD 158BW Low Density Polyethylene Resin Product Description: LD 158 series are LDPE grades, specially designed for lamination and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very low gel .. |
|||
Film Tensile Strength at Break, MD | 22.8 MPa | 3300 psi | ASTM D882 |
ExxonMobil LDPE LD 158JD Low Density Polyethylene Resin Product Description: LD 158 series are LDPE grades, specially designed for lamination and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very low gel .. |
|||
Film Tensile Strength at Break, MD | 22.8 MPa | 3310 psi | |
Dow LDPE 768A Low Density Polyethylene, Film Grade DOW LDPE 768A resin is a medium density film resin with additional stabilization for films requiring high modulus such as paper overwrap. It contains low levels of both slip additive and antiblock a.. |
|||
Film Tensile Strength at Break, MD | 22.8 MPa | 3310 psi | ASTM D-882 |
Bapolene® 200F Polyethylene, Film Grade Bapolene LD200F is a general purpose low density polyethylene for blown film extrusion applications. It contains medium levels of slip/antiblock additives. This product meets FDA standards for foo.. |
|||
Film Tensile Strength at Break, MD | 22.8 MPa | 3310 psi | MD-TD Average; ASTM D882 |
DuPont Elvax® 3130SB Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
(discontinued **) 12 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra.. |
|||
Film Tensile Strength at Break, MD | 22.8 MPa | 3310 psi | MD-TD Average; ASTM D882 |
DuPont Elvax® 3130SBZ Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
(discontinued **) 12 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra.. |