Polymer Property : Film Tensile Strength at Break, MD = 191 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 191 MPa
27700 psi
ASTM D882A
DuPont Teijin Films Melinex® 306 Polyester Film, 300 Gauge
Melinex® 306 is a clear, smooth pretreated polyester film. Melinex® 306 is produced from a lightly filled polymer, giving it a very smooth surface. The two side chemical coating provides adhesion ..
Film Tensile Strength at Break, MD 191 MPa
27700 psi
ASTM D882A
DuPont Teijin Films Melinex® 606 Polyester Film, 300 Gauge
Melinex® 606 is a very smooth two-side coated polyester film designed specifically for high density floppy disks.Also available in 285 GaugeInformation provided by DuPont.
Film Tensile Strength at Break, MD 191 MPa
27700 psi
ASTM D882A
DuPont Teijin Films Mylar® ADS Polyester Film, 300 Gauge
Mylar® ADS is a heat stabilized, low shrinkage film with good web handling properties. Approvals: UL 94 VTM-2 - for 92 - 500 gauge (0.023 - 0.13mm)Also available in 285 GaugeInformation provided by..