Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 165 MPa | 24000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 342 Polyester Film Melinex® 342 is a two-side heat-sealable, clear polyester film which is ideal in specialty card laminate applications. This film can be heat sealed to itself and other polyesters, as well as a vari.. |
|||
Film Tensile Strength at Break, MD | 165 MPa | 24000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 561 Polyester Film Melinex® 561 is a high clarity polyester film which is pretreated on both sides to promote adhesion to many industrial coatings and inks. Melinex® 561 is suitable for applications which require a .. |
|||
Film Tensile Strength at Break, MD | 165 MPa | 24000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 725 Polyester Film Melinex® 725 is a high clarity polyester film pretreated on both sides to promote adhesion to many industrial coatings and inks. Melinex® 725 exhibits improved performance in multi-pass printing a.. |
|||
Film Tensile Strength at Break, MD | 165 MPa | 24000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 965 Polyester Film, 500 Gauge Melinex® 965 is a slightly hazy film with internal UV blocker. It is pretreated on one surface to promote adhesion to many solvent systems. It has a superb web handleability.Information provided by.. |
|||
Film Tensile Strength at Break, MD | 165 MPa | 24000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 966 Polyester Film, 700 Gauge Melinex® 966 is a slightly hazy film with internal UV blocker. It is pretreated on one surface to promote adhesion to many solvent systems. It has a superb web handleability.Information provided by.. |
|||
Film Tensile Strength at Break, MD | 165 MPa | 24000 psi | ASTM D882A |
DuPont Teijin Films Mylar® EC Polyester Film, 300 Gauge Mylar® EC films are electrical grade films designed for use in applications where improved dimensional stability is required. In addition to lower levels of shrinkage, Mylar® EC films offer outsta.. |
|||
Film Tensile Strength at Break, MD | 165 MPa | 24000 psi | ASTM D882A |
DuPont Teijin Films Mylar® EC Polyester Film, 400 Gauge Mylar® EC films are electrical grade films designed for use in applications where improved dimensional stability is required. In addition to lower levels of shrinkage, Mylar® EC films offer outsta.. |
|||
Film Tensile Strength at Break, MD | 165 MPa | 24000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 943 Polyester Film Melinex® 943 is a super clear film with internal UV blocker. It is pretreated on one surface to promote adhesion to many solvent systems.Information provided by DuPont. |
|||
Film Tensile Strength at Break, MD | 165 MPa | 23900 psi | ASTM D882 |
DuPont Teijin Films Mylar® MC2 Polyester Film, 50 Gauge (14 µm), PVDC Coated Data provided by DuPont Packaging Polymers.A polyester film with a vacuum deposited layer of aluminum on one side and overcoated on both sides with a heat sealable PVDC copolymer. The film has exce.. |