Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 13.0 MPa
1890 psi
ISO 527-3
Polimeri Europa Clearflex® CH G0 Very Low Density Polyethylene
Clearflex CH G0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin has an excellent compatibility with polyolefins and fillers.Main Applic..
Film Tensile Strength at Break, MD 13.0 MPa
1890 psi
ASTM D3759
3M Scotch® 355 Superior Performance Box Sealing Tape
Scotch® Box Sealing Tape 355 is a superior performance packaging tape used for box sealing, splicing, recouperage and other demanding packaging applications. This product has a strong abrasion resi..
Film Tensile Strength at Break, MD 13.0 - 76.6 MPa
1890 - 11100 psi
Average value: 46.6 MPa Grade Count:12
Overview of materials for Very Low Density Polyethylene (VLDPE)
This property data is a summary of similar materials in the MatWeb database for the category "Very Low Density Polyethylene (VLDPE)". Each property range of values reported is minimum and maximum va..