Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 70 g | 70 g | Coextruded Film; ASTM D1922 |
Total HDPE 6420 High Density Polyethylene, Film Resin Polyethylene: Medium molecular weight, high density film resinCharacteristics:Excellent moisture barrier propertiesLow gelsLow taste and odorHigh stiffnessGood processabilityGood compatibility with.. |
|||
Elmendorf Tear Strength MD | 70 g | 70 g | ASTM D1922 |
Westlake EMAC® SP2255 17% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2255 is a 17% EMA copolymer containing slip and antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat s.. |
|||
Elmendorf Tear Strength MD | 70 g | 70 g | ASTM D1922 |
ExxonMobil LLDPE LL 1107X93 Linear Low Density Polyethylene Resin Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr.. |
|||
Elmendorf Tear Strength MD | 70 g | 70 g | ASTM D1922 |
ExxonMobil LLDPE LL 1107X95 Linear Low Density Polyethylene Resin Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr.. |
|||
Elmendorf Tear Strength MD | 70 g | 70 g | ASTM D1922 |
ExxonMobil Pax-Plus™ 3201 Blown Film Resin Pax-Plus 3201 is a rubber modified high density polyethylene film resin that exhibits excellent impact strength and stress crack resistance. It is used primarily in film where its good tear resista.. |
|||
Elmendorf Tear Strength MD | 70 g | 70 g | ASTM D1922 |
ExxonMobil Pax-Plus™ 3208 Blown Film Resin Pax-Plus 3208 is a rubber modified high density polyethylene film resin offering good physical properties with ease of processing. It exhibits toughness, stress crack resistance and low WVTR.Inform.. |
|||
Elmendorf Tear Strength MD | 70 g | 70 g | |
Dow DOWLEX™ 2037 Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2037 Polyethylene is a cast film extrusion resin for high stiffness film applications. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2a when used unmodified and according to good.. |
|||
Elmendorf Tear Strength MD | 70 g | 70 g | gF; ASTM D1922 |
Braskem LF0720/21AF Blown Film Extrusion Linear Low Density Polyethylene Description: LF0720/21AF is a LLDPE Butene copolymer produced using Unipol® process technology. It shows low haze and high clarity associated with good balance of mechanical properties, processing .. |
|||
Elmendorf Tear Strength MD | 70 g | 70 g | ASTM D1922 |
ExxonMobil Exceed™ 3527PA Metallocene Polyethylene Resin Product Description: Exceed 3527PA is a metallocene ethylene-hexene copolymer. Films made from Exceed 3527PA have high modulus and outstanding tensile, impact and puncture resistance properties. The.. |