Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 56 g | 56 g | Orientation not specified; ASTM D1922 |
Nylene® 615 Nylon 6, Film Grade Film Grade. Nylene 615 is an extrusion grade nylon 6 resin suitable for coating and film co-extrusion applications. It has excellent melt stability and good melt strength. Nylene 615 has superior
.. |
|||
Elmendorf Tear Strength MD | 56 g | 56 g | Orientation not specified; ASTM D1922 |
Nylene® 615I Nylon 6, Film Grade Film Grade. Nylene 615I is an extrusion grade nylon 6 resin suitable for film co- extrusion applications and blown film. It has excellent melt stability and good melt strength. Nylene 615I has supe.. |
|||
Elmendorf Tear Strength MD | 56 g | 56 g | Orientation not specified; ASTM D1922 |
Nylene® 615SA Nylon 6, Film Grade Film Grade. Nylene 615SA is a Kosher, extrusion grade nylon 6 resin suitable for film co-extrusion applications and blown film. It has excellent melt stability and good melt strength. Nylene
615SA.. |
|||
Elmendorf Tear Strength MD | 56 g | 56 g | Orientation not specified; ASTM D1922 |
Nylene® NX3055I Nylon 6 Dry as molded. Film Grade. Nylene NX3055I is an extrusion grade nylon 6 suitable for cast film, blown film, and co-extrusion applications. NX3055I is highly crystalline which yields excellent roll.. |
|||
Elmendorf Tear Strength MD | 56 g | 56 g | Orientation not specified; ASTM D1922 |
Nylene® NX3411 Nylon 6 Film Grade. Nylene NX3411 is an extrusion grade nylon 6 resin suitable for film co-extrusion applications and blown film. It has excellent melt stability and good melt strength. Nylene NX3411 has
.. |