Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 200 g | 200 g | ASTM D1922 |
SABIC 6318B Linear Low Density Polyethylene for Cast Film Product Description: 6318B is a hexene copolymer Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high process.. |
|||
Elmendorf Tear Strength MD | 200 g | 200 g | ASTM D1004 |
DuPont™ Sclairfilm® MPP-1 LLDPE Film, "Super Strength", 25 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.An oriented linear low density polyethylene (LLDPE) sealant film that combines exceptional strength and flex-crack characteristics with the outstanding hea.. |
|||
Elmendorf Tear Strength MD | 200 g | 200 g | ASTM D1004 |
DuPont™ Sclairfilm® MPP-3 LLDPE Film, "Super Strength", 25 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.An oriented linear low density polyethylene (LLDPE) sealant film that combines exceptional strength and flex-crack characteristics with the outstanding hea.. |
|||
Elmendorf Tear Strength MD | 200 g | 200 g | ASTM D1922 |
ExxonMobil Escorene® LL-3023 LLDPE/Hexene Premium Cast Stretch Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3023 have outstanding tensile properties as well as stiffness and toughness.Applicatio.. |
|||
Elmendorf Tear Strength MD | 200 g | 200 g | ASTM D1922 |
NOVA Chemicals Novapol® LF-Y824-C LDPE Clarity Film Resin
(discontinued **) Features: High optical clarityExcellent processabilityExcellent shrink film characteristics Applications: High clarity shrink filmProduce and bakery filmTextile packaging filmInformation provided by.. |
|||
Elmendorf Tear Strength MD | 200 g | 200 g | ASTM D1922 |
LyondellBasell Plexar® PX3236 Extrudable Tie-Layer Resin - Anhydride Modified LLDPE General DescriptionPLEXAR tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins a.. |
|||
Elmendorf Tear Strength MD | 200 g | 200 g | ISO 6383/2 |
Borealis Borstar® FB1350 Medium Density Polyethylene Borstar® FB1350 is a linear medium density polyethylene grade combining excellent extrusion properties with high film stiffness. Borstar® FB1350 is well suited for mono- and coextrusion of films .. |
|||
Elmendorf Tear Strength MD | 200 g | 200 g | ASTM D1922 |
ExxonMobil Exceed™ 1012HA Metallocene Polyethylene Resin Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymer. Films made from these resins have outstanding cold temperature toughness, impact strength and puncture. Thes.. |
|||
Elmendorf Tear Strength MD | 200 g | 200 g | ASTM D1922 |
ExxonMobil Exceed™ 1327CA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1327CA is a metallocene ethylene-hexene copolymers. It produces films which have high modulus whilst retaining good toughness. These properties together with excellent dr.. |
|||
Elmendorf Tear Strength MD | 200 g | 200 g | ASTM D1922 |
ExxonMobil LD 312.09 High Impact Film Resin LD 312 Series films have superior impact strength, good heat sealability, and good low temperature properties. Applications include frozen and other food packaging.Information provided by ExxonMobi.. |
|||
Elmendorf Tear Strength MD | 200 g | 200 g | ASTM D1922 |
ExxonMobil LD 312.23 High Impact Film Resin LD 312 Series films have superior impact strength, good heat sealability, and good low temperature properties. Applications include frozen and other food packaging.Information provided by ExxonMobi.. |
|||
Elmendorf Tear Strength MD | 200 g | 200 g | ASTM D1922 |
ExxonMobil LD 312.82 High Impact Film Resin LD 312 Series films have superior impact strength, good heat sealability, and good low temperature properties. Applications include frozen and other food packaging.Information provided by ExxonMobi.. |
|||
Elmendorf Tear Strength MD | 200 g | 200 g | ASTM D1922 |
ExxonMobil LDPE LD 104BR Low Density Polyethylene Resin Product Description: LD 104BR is an LDPE grade, which offers good optical properties combined with increased stiffness.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antibloc.. |
|||
Elmendorf Tear Strength MD | 200 g | 200 g | ASTM D1922 |
ExxonMobil LDPE LD 150AC Low Density Polyethylene Resin Product Description: LD 150 series are LDPE grades, offering good blend mechanical properties and stiffness. Several additive packages are available according to the required surface properties.Avai.. |
|||
Elmendorf Tear Strength MD | 200 g | 200 g | ASTM D1922 |
ExxonMobil LDPE LD 150BW Low Density Polyethylene Resin Product Description: LD 150 series are LDPE grades, offering good blend mechanical properties and stiffness. Several additive packages are available according to the required surface properties.Avai.. |
|||
Elmendorf Tear Strength MD | 200 g | 200 g | ASTM D1922 |
ExxonMobil LDPE LD 157CW Blown Low Density Polyethylene Resin Product Description: LD 157CW offer good mechanical properties as well as excellent opticals.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: YesAppl.. |
|||
Elmendorf Tear Strength MD | 200 g | 200 g | ASTM D1922 |
ExxonMobil LDPE LD 158BW Low Density Polyethylene Resin Product Description: LD 158 series are LDPE grades, specially designed for lamination and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very low gel .. |
|||
Elmendorf Tear Strength MD | 200 g | 200 g | ASTM D1922 |
ExxonMobil LDPE LD 158JD Low Density Polyethylene Resin Product Description: LD 158 series are LDPE grades, specially designed for lamination and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very low gel .. |
|||
Elmendorf Tear Strength MD | 200 g | 200 g | ASTM D1922 |
ExxonMobil LDPE LD 171BA Low Density Polyethylene Resin (European Grade) Product Description: LD 171BA is an LDPE grade, which offers good film rigidity combined with very good optical properties.Availability: Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: No.. |
|||
Elmendorf Tear Strength MD | 200 g | 200 g | ASTM D1922 |
ExxonMobil LDPE LD 313.NF Low Density Polyethylene Resin Product Description: LD 313.NF is a 3 % vinyl acetate copolymer. The vinyl acetate content of this resin provides good heat sealing and good cold temperature toughness when compared to LDPE homopoly.. |
|||
Elmendorf Tear Strength MD | 200 g | 200 g | ASTM D1922 |
ExxonMobil Nexxstar™ NX-00328 Low Density Polyethylene Resin Product Description: Nexxstar 00328 is an LDPE grade, which offers good film rigidity combined with very good optical properties. Its primary use is for high performance collation shrunk packaging.A.. |
|||
Elmendorf Tear Strength MD | 200 g | 200 g | ASTM D1922 |
ExxonMobil Exceed™ 1012HJ Metallocene Polyethylene Resin Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymer. Films made from these resins have outstanding cold temperature toughness, impact strength and puncture. Thes.. |
|||
Elmendorf Tear Strength MD | 200 g | 200 g | ASTM D1922 |
3M 6143 Heavy Duty Water Activated Paper Tape 3M™ Heavy Duty Water Activated Paper Tape 6142 is used for box sealing and other packaging applications. This product has a paper backing and a gummed, high tack, water-activated, modified cornstar.. |
|||
Elmendorf Tear Strength MD | 200 g | 200 g | |
Westlake Hifor SC74560-F Clear Polyethylene
(discontinued **) Hifor Clear Polyethylene SC74560-F polymer is a high strength and high clarity polyethylene designed for blown film extrusion that contains medium slip and medium antiblock additives. Films produc.. |