Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 170 g | 170 g | ASTM D1922 |
ExxonMobil Escorene® LL-3001 LLDPE/Hexene Premium Film Resin, Tough, 0.6 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE film resin. Films made from LL-3001 have outstanding tensile and toughness properties. The superior strength properties a.. |
|||
Elmendorf Tear Strength MD | 170 g | 170 g | ASTM D1922 |
LyondellBasell Petrothene® GA502022 Linear Low Density Polyethylene ApplicationsThe PETROTHENE GA 502 series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These pelletized produc.. |
|||
Elmendorf Tear Strength MD | 170 g | 170 g | ASTM D1922 |
LyondellBasell Petrothene® GA502024 Linear Low Density Polyethylene ApplicationsThe PETROTHENE GA 502 series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These pelletized produc.. |
|||
Elmendorf Tear Strength MD | 170 g | 170 g | ASTM D1922 |
LyondellBasell Petrothene® GA502023 Linear Low Density Polyethylene ApplicationsThe PETROTHENE GA 502 series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These pelletized produc.. |
|||
Elmendorf Tear Strength MD | 170 g | 170 g | ASTM D1922 |
ExxonMobil Exceed™ 1327HA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1327HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1327HA resin have excellent tensile, impact strength and puncture. These superior strength prope.. |
|||
Elmendorf Tear Strength MD | 170 g | 170 g | ASTM D1922 |
ExxonMobil LD 334.57 Clear, High Impact Film Resin LD 334 resins produce films with superior impact strength, good heat sealability, and low temperature properties.Information provided by ExxonMobil Chemical |
|||
Elmendorf Tear Strength MD | 170 g | 170 g | ASTM D1922 |
ExxonMobil LD 334.82 Clear, High Impact Film Resin LD 334 resins produce films with superior impact strength, good heat sealability, and low temperature properties.Information provided by ExxonMobil Chemical |
|||
Elmendorf Tear Strength MD | 170 g | 170 g | ASTM D1922 |
ExxonMobil LDPE LD 160AT Low Density Polyethylene Resin Product Description: LD 160 series are LDPE grades, which offer good draw down and optical properties.Availability: Africa & Middle East, Asia Pacific, Latin America, North America and South America.. |
|||
Elmendorf Tear Strength MD | 170 g | 170 g | ASTM D1922 |
Dow DOWLEX™ 2025G Linear Low Density Polyethylene DOWLEX™ 2025G is a medium modulus resin with excellent toughness properties designed for thin film applications.Information provided by Dow |
|||
Elmendorf Tear Strength MD | 170 g | 170 g | ASTM D1922 |
ExxonMobil Exceed™ 2718CB Premium Cast Film Resin Exceed 2718CB resin is a hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 2718CB resin have outstanding tensile properties and impact and puncture toughness.. |