Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 145 g | 145 g | ASTM D1922 |
Iran Petrochemical (PCC) LL0209AA Linear Low Density Polyethylene LL 0209AA is a LLDPE copolymer with butene as comonomer which contains anti-oxidant. It is recommended for general purpose applications.Information provided by Iran Petrochemical Commercial Co. |
|||
Elmendorf Tear Strength MD | 145 g | 145 g | ASTM-D1922 |
Braskem TN2006 EVA General Film Copolymer TN2006 is an Ethylene-Vinyl Acetate (EVA) copolymer with good mechanical properties, high flexibility and toughness even with low temperature, and excellent optical and heat sealability properties. .. |
|||
Elmendorf Tear Strength MD | 145 g | 145 g | |
Dow LDPE 535I Low Density Polyethylene, Liner Grade DOW LDPE 535I resin is a barefoot general purpose liner resin with medium clarity for medium modulus packaging applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for.. |