Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 8.83 g | 8.83 g | ASTM D1922 |
LG Chemical LUTENE FB3000 LDPE Extrusion of Blown Film Description: LUTENE FB3000 is mainly intended for the extrusion of blown film with high mechanical property for the clarity bags in all thickness. LUTENE FB3000 have high mechanical property and ena.. |
|||
Elmendorf Tear Strength MD | 8.83 - 1070 g | 8.83 - 1070 g | Average value: 316 g Grade Count:122 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |