Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 65 g | 65 g | ASTM D1922 |
SABIC 318B Linear Low Density Polyethylene for Cast Film Product Description: 318B is a Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high processing temperatures u.. |