Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 58 g | 58 g | ASTM D1922 |
Huntsman Rexell® M3104 Blown Film Extrusion LLDPE
(discontinued **) Linear-low medium density copolymer, cast film extrusion, FDA compliant.Features: Excellent combination of toughness, stiffness, and optics with good temperature resistance.Applications: Diaper film.. |
|||
Elmendorf Tear Strength MD | 58 g | 58 g | Orientation not specified; ASTM D1922-89 |
DuPont™ Kapton® 250FN029 Polyimide/FEP Composite Film 250 Gauge film structure consisting of a 50 µm (2 mil) base polyimide film with a 13 µm (0.5 mil) coating of Teflon® FEP on one side.Kapton® Type HN film coated with Teflon® FEP fluoropolymer r.. |
|||
Elmendorf Tear Strength MD | 58 g | 58 g | gF; ASTM D1922 |
Braskem Green PE SGM9450F Blow Film Extrusion and Cast Film Extrusion High Density Polyethylene Description: SGM9450F is a high-density polyethylene, developed for the high molecular weight film extrusion segment produced with bimodal technology. The film produced from this resin has high tena.. |