Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 480 g | 480 g | ASTM D1922 |
ExxonMobil LD 123.LN General Purpose Clarity Film Resin Product Description: LD 123.LN blown film grade offers an excellent balance of optical and strength properties for general purpose clear film applications.Availability: Latin America, North America .. |
|||
Elmendorf Tear Strength MD | 480 g | 480 g | ASTM D1922 |
ExxonMobil LDPE LD 123.LN Low Density Polyethylene Resin Product Description: LD 123.LN blown film grade offers an excellent balance of optical and strength properties for general purpose clear film applications.Availability: Latin America, North America .. |
|||
Elmendorf Tear Strength MD | 480 g | 480 g | ASTM D1922 |
Huntsman Rexell® L3102 Blown Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer, cast film extrusion, FDA compliant.Features: Good impact and puncture resistance with excellent optics and sealability.Applications: Laminated and coextruded films for .. |