Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 450 g | 450 g | |
Eastman E6838-922F Polyethylene
(discontinued **) E6838-922F is a low density formulation with medium slip and medium antiblock. Outstanding optical properties make this material an excellent choice for food packaging applications.List of Applicat.. |
|||
Elmendorf Tear Strength MD | 450 g | 450 g | ASTM D1922 |
ExxonMobil Escorene® LD-140 LDPE Industrial Film resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index homopolymer resin for production of film with very good toughness.Applications: Heavy duty bags. Data for film properties b.. |
|||
Elmendorf Tear Strength MD | 450 g | 450 g | ASTM D1922 |
LG Chemical SEETEC BF315 LDPE Characteristics: Good Processability and Excellent Optical PropertiesApplications: Masking filmCAS No. 9002-88-4Information provided by LG Chemical |
|||
Elmendorf Tear Strength MD | 450 g | 450 g | ASTM D1922 |
Westlake Mxsten CV77512 Polyethylene Plastomer Mxsten CV plastomer CV77512 is a polyethylene plastomer designed for blown film extrusion that contains high slip, high antiblock and high processing aid additives. Films produced with this resin ex.. |
|||
Elmendorf Tear Strength MD | 450 g | 450 g | ASTM D1922 |
Westlake Mxsten CV77523 Polyethylene Plastomer Mxsten CV plastomer CV77523 is a polyethylene plastomer designed for blown film extrusion that contains high slip, very high antiblock and polymer processing aid additives. Films produced with this .. |
|||
Elmendorf Tear Strength MD | 450 g | 450 g | |
Dow Primacor® 1430 Ethylene Acrylic Acid (EAA) Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical. |
|||
Elmendorf Tear Strength MD | 450 g | 450 g | ASTM D-1922 |
Bapolene® 152A Polyethylene Film Grade Bapolene 152A is a hexene linear low density polyethylene with a combination of superior impact strength and HSIT. Product is designed to exhibit performance similar to that of metallocene products... |
|||
Elmendorf Tear Strength MD | 450 g | 450 g | ASTM D-1922 |
Bapolene® 152B Polyethylene Film Grade Bapolene 152B is a hexene linear low density polyethylene with a combination of superior impact strength and HSIT. Product is designed to exhibit performance similar to that of metallocene products... |
|||
Elmendorf Tear Strength MD | 450 g | 450 g | ASTM D-1922 |
Bapolene® 152F Polyethylene Film Grade Bapolene 152F is a hexene linear low density polyethylene with a combination of superior impact strength and HSIT. Product is designed to exhibit performance similar to that of metallocene products... |
|||
Elmendorf Tear Strength MD | 450 g | 450 g | ASTM D1922 |
Huntsman Rexell® V3101 Blown Film Extrusion LLDPE
(discontinued **) Linear-low very low density copolymer, cast film extrusion, FDA compliant.Features: High toughness, puncture resistance with good sealing and excellent optical properties.Applications: Food packagin.. |
|||
Elmendorf Tear Strength MD | 450 g | 450 g | ASTM D1922 |
M. Holland Company MAGMA® LM124-C LLDPE
(discontinued **) Features: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Elmendorf Tear Strength MD | 450 g | 450 g | ASTM D1922 |
M. Holland Company MAGMA® LM213-C LLDPE
(discontinued **) Features: Good Heat Seal, Good Tear Strength, Good ToughnessUses: BlendingProcessing Method: ExtrusionInformation provided by M. Holland. |