Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 300 g | 300 g | ASTM D 1922 |
NOVA Chemicals Surpass® FPs117-C Octene Copolymer sLLDPE Film Resins FPs117-C complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without .. |
|||
Elmendorf Tear Strength MD | 300 g | 300 g | ASTM D1922 |
ExxonMobil Escorene® LD-113 LDPE General Purpose Packaging Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin that offers a good balance of toughness, drawdown capability, stiffness and clarity. LD-113 exhibits good machinability in.. |
|||
Elmendorf Tear Strength MD | 300 g | 300 g | Cast; ASTM D1922 |
LyondellBasell Petrothene® NA373244 Low Density Polyethylene, Cast/Blown Film Grade ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with.. |
|||
Elmendorf Tear Strength MD | 300 g | 300 g | ASTM D1922 |
LyondellBasell Petrothene® NA960000 Low Density Polyethylene ApplicationsPETROTHENE NA960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA960 exhibits good unif.. |
|||
Elmendorf Tear Strength MD | 300 g | 300 g | ASTM D1922 |
LyondellBasell Petrothene® NA960070 Low Density Polyethylene ApplicationsPETROTHENE NA 960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA 960 exhibits good un.. |
|||
Elmendorf Tear Strength MD | 300 g | 300 g | ASTM D1922 |
LyondellBasell Petrothene® NA960083 Low Density Polyethylene ApplicationsPETROTHENE NA 960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA 960 exhibits good un.. |
|||
Elmendorf Tear Strength MD | 300 g | 300 g | ASTM D1922 |
LyondellBasell Petrothene® NA963083 Low Density Polyethylene ApplicationsPETROTHENE NA 963 is a series of resins formulated with special antiblock additive and designed for a wide variety of industrial film applications where high impact strength and excellen.. |
|||
Elmendorf Tear Strength MD | 300 g | 300 g | Cast; ASTM D1922 |
LyondellBasell Petrothene® NA373242 Low Density Polyethylene, Cast/Blown Film Grade ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with.. |
|||
Elmendorf Tear Strength MD | 300 g | 300 g | ASTM D1922 |
Westlake Mxsten CV77518 Polyethylene Plastomer Mxsten CV Plastomer CV77518 resin is a polyethylene plastomer designed for blown and cast film extrusion that contains no slip and no antiblock additives. Films produced with this resin exhibit a ve.. |
|||
Elmendorf Tear Strength MD | 300 g | 300 g | ASTM D1922 |
Teknor Apex Terraloy™ BP 20001A Thermoplastic Starch + Copolyester Notes: Terraloy™ BP-20001A is a Thermoplastic Starch/Biodegradable Copolyester ready-to-process compound that contains up to 40% of TPS renewable content and is 100% biodegradable. This compound i.. |
|||
Elmendorf Tear Strength MD | 300 g | 300 g | ASTM D1922 |
ExxonMobil Exceed™ 2018CA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2018CA is a metallocene ethylene-hexene copolymer. The higher melt index makes this polymer ideally suited for blending into LDPE rich films as well as skin layer in coex.. |
|||
Elmendorf Tear Strength MD | 300 g | 300 g | ASTM D1922 |
ExxonMobil LLDPE LL 3001.32 Cast Linear Low Density Polyethylene Resin Product Description: LL 3001.32 is a hexane copolymer LLDPE designed for the blown or cast film process. Films made from LL 3001.32 have outstanding tensile and toughness properties. The superior st.. |
|||
Elmendorf Tear Strength MD | 300 g | 300 g | |
Dow AFFINITY™ PF 1140 Polyolefin Plastomer AFFINITY® PF 1140 polyolefin plastomer is an ethylene alpha-olefin resin designed for use in a variety of demanding applications including high-speed, form-fill seal products, display films and fre.. |
|||
Elmendorf Tear Strength MD | 300 g | 300 g | |
Dow AFFINITY™ PL 1850 Polyolefin Plastomer AFFINITY® PL 1850 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide blown and cast film products with low temperature sealability, excellent optics and good abuse resistanc.. |
|||
Elmendorf Tear Strength MD | 300 g | 300 g | |
Dow DOWLEX™ 2035 Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2035 Polyethylene resin is for cast film extrusion. It offers excellent tear strength, toughness and good processability. It complies with FDA regulation 21 CFR 177.1520(c) 3.2a when used u.. |
|||
Elmendorf Tear Strength MD | 300 g | 300 g | ASTM D1922 |
Dow DOWLEX™ 2085G Polyethylene Resin DOWLEX™ 2085G is an ethylene-octene copolymer designed for general purpose thin gauge film applications. It is perfect for high strength consumer trash bags/liners. This product can be used in ot.. |
|||
Elmendorf Tear Strength MD | 300 g | 300 g | |
Dow LDPE 530A Low Density Polyethylene, Blown Film Grade DOW LDPE 530A resin, is a general purpose barefoot blown film extrusion resin with excellent drawdown and processability for packaging applications. This material complies with U.S.FDA regulation 21.. |
|||
Elmendorf Tear Strength MD | 300 g | 300 g | |
Dow Primacor® 1410 Ethylene Acrylic Acid (EAA) Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical. |
|||
Elmendorf Tear Strength MD | 300 g | 300 g | gF; ASTM D1922 |
Braskem Green PE SLH118 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Description: SLH118 is a Linear Low Density Polyethylene, copolymer of hexene-1. Developed for blown film extrusion in blends with polyethylenes. Films obtained with this product show a good process.. |
|||
Elmendorf Tear Strength MD | 300 g | 300 g | ASTM 1922 |
Braskem LH 118 LLDPE Blown Film Extrusion Polyethylene Description: LH118 is a Linear Low Density Polyethylene, copolymer of hexene-1, produced by Spherilene process. Developed for blown film extrusion in blends with polyethylenes. Films obtained with t.. |
|||
Elmendorf Tear Strength MD | 300 g | 300 g | gF; ASTM D1922 |
Braskem LH118 Blown Film Extrusion Linear Low Density Polyethylene Stretch films; Liners; LDPE and HDPE blends; Packages for general use.Information provided by Braskem. |
|||
Elmendorf Tear Strength MD | 300 g | 300 g | ASTM-D1922 |
Braskem TS7003 LDPE Blown Film Extrusion Polyethylene TS7003 is a low-density polyethylene (LDPE) with high molecular weight that offers high mechanical strength and toughness even at low temperatures. Additionally, this product is easily processed. Th.. |
|||
Elmendorf Tear Strength MD | 300 g | 300 g | ISO 6283-2 |
Carmel Olefins IPETHENE® 100 Low Density Polyethylene IPETHENE® 100 is a low density polyethylene extrusion grade. It exhibits good impact and puncture resistance, good processability and good ESCR. APPLICATIONS IPETHENE® 100 is used for production.. |
|||
Elmendorf Tear Strength MD | 300 g | 300 g | |
Dow LDPE 607A Low Density Polyethylene, High Clarity Blown Film Grade DOW LDPE 607A resin is a fully formulated high clarity blown film resin for thin gauge optical applications, such as bakery film. It contains medium levels of slip additive and low levels of antiblo.. |
|||
Elmendorf Tear Strength MD | 300 g | 300 g | ASTM-D1922 |
Braskem TX7003 LDPE Blown Film Extrusion Polyethylene TX7003 is a low-density, high molecular-weight polyethylene that offers high mechanical strength. The product's characteristics allow for high versatility and use in various applications due to its .. |