Secant Modulus 0.149 GPa
21.6 ksi
0.01; ASTM D638
Braskem BI 818 LDPE Injection Molding Polyethylene  (discontinued **)
Applications: Injection molding; masterbatches. Information provided by Braskem
Secant Modulus 0.149 - 1.45 GPa
21.6 - 210 ksi
Average value: 0.279 GPa Grade Count:18
Overview of materials for Low Density Polyethylene (LDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum ..