Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® LBT-2 Polyester Packaging Film, 48 Gauge Data provided by DuPont Packaging Polymers.Mylar® LBT-2 is an uncoated, transparent, exceptionally strong film used as a substrate for laminating and extrusion coating and as a component of packagi.. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® LBT-2 Polyester Packaging Film, 92 Gauge Data provided by DuPont Packaging Polymers.Mylar® LBT-2 is an uncoated, transparent, exceptionally strong film used as a substrate for laminating and extrusion coating and as a component of packagi.. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® OB12 Polyester Packaging Film, 100 Gauge Data provided by DuPont Packaging Polymers.Mylar® OB12 is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and polyvinylidene chloride (PVDC) layer on the oppo.. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® OB12AF Polyester Packaging Film, 50 Gauge Data provided by DuPont Packaging Polymers.Mylar® OB12AF is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and polyvinylidene chloride (PVDC) layer on the op.. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® OL12 Polyester Packaging Film, 100 Gauge Data provided by DuPont Packaging Polymers.Mylar® OL12 (formerly known as XM963A) is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat sea.. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® OL12 Polyester Packaging Film, 150 Gauge Data provided by DuPont Packaging Polymers.Mylar® OL12 (formerly known as XM963A) is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat sea.. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® OL12 Polyester Packaging Film, 50 Gauge Data provided by DuPont Packaging Polymers.Mylar® OL12 (formerly known as XM963A) is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat sea.. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® OL13 Polyester Packaging Film, 100 Gauge Data provided by DuPont Packaging Polymers.Mylar® OL13 (formerly known as XM110) is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat seal.. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® OL13 Polyester Packaging Film, 150 Gauge Data provided by DuPont Packaging Polymers.Mylar® OL13 (formerly known as XM110) is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat seal.. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® RL32 Polyester Packaging Film, 100 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL32 (formerly known as XM999) is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a .. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® RL32 Polyester Packaging Film, 150 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL32 (formerly known as XM999) is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a .. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® RL32 Polyester Packaging Film, 50 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL32 (formerly known as XM999) is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a .. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® RL33 Polyester Packaging Film, 100 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL33 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film.. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® RL33 Polyester Packaging Film, 150 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL33 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film.. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® RL33 Polyester Packaging Film, 50 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL33 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film.. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® RL4 Polyester Packaging Film, 100 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL4 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film .. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® RL4 Polyester Packaging Film, 50 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL4 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film .. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® RL4 Polyester Packaging Film, 75 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL4 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film .. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® RL42 Polyester Packaging Film, 100 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL42 (formerly known as XM985) is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a .. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® RL42 Polyester Packaging Film, 150 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL42 (formerly known as XM985) is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a .. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® RL42 Polyester Packaging Film, 50 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL42 (formerly known as XM985) is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a .. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® RL42 Polyester Packaging Film, 75 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL42 (formerly known as XM985) is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a .. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® RL43 Polyester Packaging Film, 100 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL43 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. Mylar® RL43 is designed to produce stro.. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® RL43 Polyester Packaging Film, 150 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL43 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. Mylar® RL43 is designed to produce stro.. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® RL43 Polyester Packaging Film, 50 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL43 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. Mylar® RL43 is designed to produce stro.. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® OB01 Polyester Packaging Film, 50 Gauge Data provided by DuPont Packaging Polymers.Mylar® OB01 (formerly known as XM924) is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and a polyvinylidene chlor.. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® OB12 Polyester Packaging Film, 150 Gauge Data provided by DuPont Packaging Polymers.Mylar® OB12 is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and polyvinylidene chloride (PVDC) layer on the oppo.. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® OB12 Polyester Packaging Film, 50 Gauge Data provided by DuPont Packaging Polymers.Mylar® OB12 is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and polyvinylidene chloride (PVDC) layer on the oppo.. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® OB12AF Polyester Packaging Film, 100 Gauge Data provided by DuPont Packaging Polymers.Mylar® OB12AF is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and polyvinylidene chloride (PVDC) layer on the op.. |
|||
Secant Modulus | 3.79 GPa | 550 ksi | Stiffness Modulus; ASTM D882 |
DuPont Teijin Films Mylar® LBT-2 Polyester Packaging Film, 75 Gauge Data provided by DuPont Packaging Polymers.Mylar® LBT-2 is an uncoated, transparent, exceptionally strong film used as a substrate for laminating and extrusion coating and as a component of packagi.. |