Polymer Property : Secant Modulus = 0.650 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 0.650 GPa
94.3 ksi
ASTM D882
Nylene® 615 Nylon 6, Film Grade
Film Grade. Nylene 615 is an extrusion grade nylon 6 resin suitable for coating and film co-extrusion applications. It has excellent melt stability and good melt strength. Nylene 615 has superior ..
Secant Modulus 0.650 GPa
94.3 ksi
ASTM D882
Nylene® 615I Nylon 6, Film Grade
Film Grade. Nylene 615I is an extrusion grade nylon 6 resin suitable for film co- extrusion applications and blown film. It has excellent melt stability and good melt strength. Nylene 615I has supe..
Secant Modulus 0.650 GPa
94.3 ksi
ASTM D882
Nylene® 615SA Nylon 6, Film Grade
Film Grade. Nylene 615SA is a Kosher, extrusion grade nylon 6 resin suitable for film co-extrusion applications and blown film. It has excellent melt stability and good melt strength. Nylene 615SA..
Secant Modulus 0.650 GPa
94.3 ksi
ASTM D882
Nylene® NX3055I Nylon 6
Dry as molded. Film Grade. Nylene NX3055I is an extrusion grade nylon 6 suitable for cast film, blown film, and co-extrusion applications. NX3055I is highly crystalline which yields excellent roll..
Secant Modulus 0.650 GPa
94.3 ksi
ASTM D882
Nylene® NX3411 Nylon 6
Film Grade. Nylene NX3411 is an extrusion grade nylon 6 resin suitable for film co-extrusion applications and blown film. It has excellent melt stability and good melt strength. Nylene NX3411 has ..
Secant Modulus 0.650 GPa
94.3 ksi
Average value: 0.650 GPa Grade Count:6
Overview of materials for Nylon 6, Film Grade