Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 33.0 MPa | 4790 psi | ASTM D882 |
SABIC F00952 High Density Polyethylene for Blown Film Product Description: F00952 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Film Tensile Strength at Yield, MD | 33.0 MPa | 4790 psi | ASTM D882 |
SABIC F00952EQ High Density Polyethylene for Blown Film Product Description: F00952EQ is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. the design of the product, molecular architect.. |
|||
Film Tensile Strength at Yield, MD | 33.0 MPa | 4790 psi | ASTM D882 |
SABIC FJ00952 High Density Polyethylene for Blown Film Product Description: FJ00952 is a TNPP additive free, high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, .. |
|||
Film Tensile Strength at Yield, MD | 33.0 MPa @Thickness 0.400 mm |
4790 psi @Thickness 0.0157 in |
ISO 527 |
Premix Thermoplastics PRE-ELEC® PS 1331 Carbon Black Filled Conductive Thermoplastic Compound PRE-ELEC® PS 1331 is a carbon black filled conductive thermoplastic compound based on polystyrene. In addition to a low electrical resistivity PRE-ELEC® PS 1331 has excellent mechanical properties.. |
|||
Film Tensile Strength at Yield, MD | 33.0 MPa | 4790 psi | ASTM D882 |
Eastman 1810F Polyethylene
(discontinued **) Polyethylene 1810F is a fractional-melt low-density formulation with no slip or antiblock. It is suggested for film applications requiring high impact strength, high tear strength and very good opt.. |
|||
Film Tensile Strength at Yield, MD | 33.0 MPa | 4790 psi | ASTM D882 |
Eastman D4004-F Polyethylene
(discontinued **) Polyethylene D4004-F is a fractional melt formulation designed for film applications. It is suggested for applications requiring toughness, clarity, high strength, and for blending with LLDPEList o.. |
|||
Film Tensile Strength at Yield, MD | 33.0 MPa | 4790 psi | ASTM D882 |
Eastman D4008-F Polyethylene
(discontinued **) Polyethylene D4008-F is a fractional melt formulation designed for film applications. It is suggested for applications requiring toughness and clarityList of Applications: Food packagingFood-contac.. |
|||
Film Tensile Strength at Yield, MD | 33.0 MPa | 4790 psi | ASTM D882 |
Eastman E6838-969F Polyethylene
(discontinued **) E6838-969F is a low density formulation with no slip and medium antiblock. It is suggested for film applications that require toughness such as shrink/bundling film, disposable diapersand overwrap... |
|||
Film Tensile Strength at Yield, MD | 33.0 MPa | 4790 psi | parallel; ISO 527-3 |
DSM Akulon® XP36-C1 PA6 Film Extrusion, Medium Viscosity, Lubricated |
|||
Film Tensile Strength at Yield, MD | 33.0 MPa | 4790 psi | parallel; ISO 527-3 |
DSM Akulon® XP32-C1 PA6 Film Extrusion, Medium Viscosity, Lubricated |
|||
Film Tensile Strength at Yield, MD | 33.0 MPa | 4790 psi | ASTM D882 |
Eastman D4052-F Polyethylene
(discontinued **) D4052-F is a fractional-melt low density formulation with low slip and low antiblock. It is suggested for film applications requiring impact strength, outstanding clarity, and good tear resistance... |
|||
Film Tensile Strength at Yield, MD | 33.0 MPa | 4790 psi | ASTM D882 |
ExxonMobil Escorene® HD-7835 MMW-HDPE Blown Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A medium molecular weight HDPE blown film resin. Films made from the HD-7835 exhibit an excellent stiffness balance. HD-7835 is particularly recom.. |