Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 26.9 MPa | 3900 psi | ASTM D882 |
ExxonMobil Escorene™ LD 706.15 Cast Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 706.15 is a 14.9 wt% vinyl acetate copolymer film resin designed for coextruded cast film applications.Availability: Latin America, North America and South Ame.. |