Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 26.5 MPa | 3840 psi | ASTM D882 |
Reliance Industries Relene F46003 Polyethylene Relene F46003 is a High Density Polyethylene grade suitable for producing blown parts with superior stiffness and barrier properties. It is recommended for making liners and coextruded film structu.. |