Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 22.8 MPa | 3300 psi | ASTM D822 |
LyondellBasell Alathon® M6020 High Density Polyethylene ApplicationsALATHON 6020 is a medium molecular high density weight homopolymer for use in blown or cast film applications. This resin provides extremely low gel content and high stiffness. Typica.. |