Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 17.0 MPa | 2470 psi | ISO 527-3 |
Polimeri Europa Flexirene® CM 50 Butene Copolymer Linear Low Density Polyethylene Flexirene CM 50 is a butene copolymer with medium density (C4-LLDPE), with antioxidants, suitable for cast film extrusion.Main Applications: Flexirene CM 50 is a highly stiff product and it is reco.. |
|||
Film Tensile Strength at Yield, MD | 17.0 MPa | 2470 psi | ASTM D882 |
NOVA Chemicals Sclair® 14G Butene LMDPE Film Resin Film Properties. Features: Low gel, good opacity, easy processability.Applications: Overwrap film.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, MD | 17.0 MPa | 2470 psi | ASTM D882 |
ExxonMobil Escorene® LD-103 LDPE Industrial Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer industrial film resin with excellent toughness. LD-103 has a low melt index which gives excellent impact strength and melt strength o.. |
|||
Film Tensile Strength at Yield, MD | 17.0 MPa | 2470 psi | ASTM D882 |
NOVA Chemicals Sclair® 14B3 Butene LMDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, good clarity, heat resistance and barrier properties.Applications: Lamination, co-extrusion.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, MD | 17.0 MPa | 2470 psi | ASTM D882 |
NOVA Chemicals Sclair® 14L1 Octene LMDPE Film Resin
(discontinued **) Low gel, Good clarity, Excellent sealing characteristicsApplications: Lamination, Co-extrusionAdditives: Process stabilizer, polymer process aidFilm properties are typical of blown film extruded at .. |
|||
Film Tensile Strength at Yield, MD | 17.0 MPa | 2470 psi | |
UBE 7024B Five Layer Film Specialties: High transparencyGood thermoform-abilityLow W.V.T.R High shrink-abilityLower extrusion temperatureProcessing: Best match for co-extrusion with EVOH resins.Typical Applications: Cereal .. |
|||
Film Tensile Strength at Yield, MD | 17.0 MPa | 2470 psi | ASTM D882 |
NOVA Chemicals Novapol® TF-0242-E Hexene LLDPE Film Resin
(discontinued **) Excellent stiffness and glossApplications: Diaper back sheet, BlendingFilm properties are typical of film extruded at 270°C.Information provided by NOVA Chemicals. |
|||
Film Tensile Strength at Yield, MD | 17.0 MPa | 2470 psi | ASTM D882 |
NOVA Chemicals Sclair® 14B1 Butene LMDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, good clarity, heat resistance and barrier properties.Applications: Lamination, co-extrusion.Data provided by the manufacturer. |