Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
Polimeri Europa Clearflex® H&T LFH 208 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LFH 208 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T LFH.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
Polimeri Europa Clearflex® H&T LFH 238 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LFH 238 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion. It contains slip and antiblocking a.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
SABIC 118 Series Linear Low Density Polyethylene for Blown Film Product Description: 118 series resins are Linear Low Density Polyethylene grades suitable for general purpose packaging. Films produced using these resins yield good tensile properties, impact st.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
SABIC 120W Linear Low Density Polyethylene for Blown Film Product Description: 120W is a Linear Low Density Polyethylene grade suitable for general purpose packaging. Films produced using this resin yield good tensile properties, impact strength and opti.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
Polimeri Europa Riblene® FC 30 Low Density Polyethylene - Blown Film Extrusion Riblene FC 30 is a high molecular weight low density polyethylene resin (LDPE) suitable for blown film extrusion. Riblene FC 30 is characterized by a high melt strength leading to a good bubble sta.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
Polimeri Europa Riblene® FF 24 Low Density Polyethylene - Blown Film Extrusion Riblene FF 24 is a high molecular weight low density polyethylene (LDPE), with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FF 24 is characterized by a good melt s.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
Polimeri Europa Riblene® FF 30 Low Density Polyethylene - Blown Film Extrusion Riblene FF 30 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 30 is characterized by a good melt strength leading to a good bubble stabilit.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
Polimeri Europa Riblene® FL 20 Low Density Polyethylene - Blown Film Extrusion Riblene FL 20 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FL 20 is characterized by a good balance between processability and mechanical properties.Films manufac.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
Polimeri Europa Riblene® FM 23 Low Density Polyethylene - Blown Film Extrusion Riblene FM 23 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FM 23 is characterized by a good balance between processabilit.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® LA-0219-A LDPE Foam Resin Features: Good heat sealing latitudeModerate toughnessEasy processability Applications: Industrial packagingLinersBlends with LLDPEFoam ArticlesInformation provided by Nova Chemicals |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® LA-0219-AM LDPE Foam Resin Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blo.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0219-A LDPE Film Resin Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinInformation provided by NOVA Chemi.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0323-A LDPE Film Resin Film Properties. Features: General purpose clarity, good heat sealing latitude, easy processability, good drawdown.Applications: Food wrap, consumer packaging, liners, blends with LLDPE.Data provid.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® PF-Y821-CP Butene LLDPE Film Resin Film Properties. Features: Good stiffness and machinability, suitable for narrow die gaps.Applications: Industrial packaging, heavy duty sacks.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® TD-9022-C Superhexene LLDPE Puncture value is 60 J/mm. Additive Package: Antiblock.Applications: industrial liners, heavy duty packaging.Film properties are typical of 25 µm blown film extruded at a blow-up ratio of 2.5:1, b.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® TF-0119-D Hexene LLDPE Film Resin Film Properties. Features: Exceptional toughness, high strength with thin films.Applications: Thin films, premium trash bags, ice bags.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Sclair® FP120-D Octene LLDPE Film Resin Applications: Food packaging, freezer film, lamination and sealant filmInformation provided by Nova Chemicals |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
SABIC HP0722N Low Density Polyethylene for Blown Film Product Description: HP0722N is a Low Density Polyethylene grade suitable for producing medium duty films and contains no slip or antiblock additives. It yields good toughness and optical properti.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
Iran Petrochemical (PCC) Arak 1209AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® LA-0218-AF LDPE Foam Resin
(discontinued **) Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Base resinFilm properties are typical of blown fi.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D 882 |
NOVA Chemicals Novapol® PF-0218-B Butene Copolymer LLDPE Film Resin PF-0218-B complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatur.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D 882 |
NOVA Chemicals Novapol® PF-0218-E Butene Copolymer LLDPE Film Resin PF-0218-E complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatur.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
Iran Petrochemical (PCC) LL0220KJ Linear Low Density Polyethylene LL0220KJ are linear low density polyethylene copolymers containing butane-1 as the comonomer.Applications: shipping sacks, carrier and garbage bags, consumer packaging, high clarity film, agricultu.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882-02 |
Ipiranga Petrochem LB 0316 LLDP IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 1184 |
SIDPEC EGYPTENE® LL 0220 AA LLDPE Film Applications:Light and medium duty filmStretch filmFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor o.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 1184 |
SIDPEC EGYPTENE® LL 0205 AF LLDPE Film Applications:Heavy duty sacks, mulch filmsStretch film, liners, geomembraneFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l... |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | |
Dow LDPE 527A Low Density Polyethylene, Blown Film Grade DOW LDPE 527A is a general purpose blown film extrusion resin for use in medium duty liner film applications and other packaging applications. It contains high levels of antiblock additive. This mat.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Sclair® 11G1 LLDPE Film Resin
(discontinued **) Low gel, Excellent seal characteristics, Easy processabilityApplications: Premium shrink film, Co-extrusionAdditives: Process stabilizer, Polymer process aidFilm properties are typical of blown film.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Sclair® 11M1 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, strength and toughness.Applications: Co-extrusion.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Sclair® 11N1 PE Film Resin